TAIRILAC® AC3600-AF PC Resin Self Extinguishing Grade
TAIRILITE PC Resin AC3600-AF is a high-flow, non-transparent polycarbonate raw material. This halogen-free (Cl/Br/Sb-free), flame-retardant material delivers exceptional impact resistance and thermal stability, ideal for precision-molded components requiring safety compliance and reliability.
- Character: High flow, Non-transparency, Cl, Br, Sb free, Flame retardant
- Application: Transformer case, Battery case, Projector housing, Electroomechanical appliance cover
Key technical data (ISO)
- Melt Flow Index: 10 g/10 min (300°C, 1.2 kg)
- Impact Strength: 735 J/m (23°C)
- Heat Resistance: 113°C HDT (1.8 MPa)
- Flexural Strength: 99 MPa | Flexural Modulus: 2,150 MPa
- Tensile Strength: 67 MPa
- Molding Shrinkage: 0.5–0.7%
- Flame Rating: UL94 V-0 (1–3 mm), V-1 (0.8 mm), V-2 (0.6 mm)
- Specific Gravity: 1.19
- Pre-Drying: 110–120°C × 4–6 hrs
- Screw Temp: 260–295°C
- Injection Pressure: 50–130 kg/cm²
- Mold Temp: 80–100°C
Features & Benefits

Application

Related Tairilite® PC Plastics
FCFC Formosa TAIRILITE® AC2916
FCFC Formosa TAIRILITE® AC2955
FCFC Formosa TAIRILITE® AC9830
FCFC Formosa TAIRILITE® AC9144
FCFC Formosa TAIRILITE® AC9140
FCFC Formosa TAIRILITE® AC2820
FCFC Formosa TAIRILITE® AC2854
FCFC Formosa TAIRILITE® AC2856
FCFC Formosa TAIRILITE® AC3873
FCFC Formosa TAIRILITE® AC3832
FCFC Formosa TAIRILITE® AC3854
FCFC Formosa TAIRILITE® AC3853
FCFC Formosa TAIRILITE® AC3843
FCFC Formosa TAIRILITE® AC3630
FCFC Formosa TAIRILITE® AC3600-AF
FCFC Formosa TAIRILITE® AC3600
FCFC Formosa TAIRILITE® AC3900
FCFC Formosa TAIRILITE® AC3839
Advanced Manufacturing