FCFC Formosa TAIRILITE® AC3630

FCFC Plastics TAIRILITE PC Resin

TAIRILAC® AC3600 PC Resin Self Extinguishing Grade

Tairilite AC3630 is a self-extinguishing grade Polycarbonate PC Resin. Combining halogen-free flame retardancy, high flow, non-transparency, and UL weather resistance certification, it delivers unmatched safety and durability. Ideal for industries prioritizing reliability and compliance.

  • Character: Halogen free, Flame retardant, High flow, Non-transparency,UL weather resistance certification
  • Application: Household appliances, 3C electronic products , outdoor equipment shell, electric bike battery case, Energy storage device
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ISO)

  • Melt Flow Index: 25 g/10 min (300°C, 1.2 kg)
  • Impact Strength: 635 J/m (IZOD), 55 kJ/m² (Charpy)
  • Tensile Strength: 66 MPa
  • Heat Resistance HDT @109°C (1.8 MPa)
  • Heat Resistance Vicat Softening: @116°C
  • Flame Rating: UL-94 V-0 (0.8–3 mm), 5VB (1.5–3 mm)
  • Molding Shrinkage: 0.5–0.7%
  • Specific Gravity: 1.19

Features & Benefits

Superior Flame Retardancy

Halogen-free and UL94 V-0/5VB rated, AC3630 eliminates toxic fumes during combustion. This ensures safer electronics and compliance with global environmental regulations.

High-Flow Processing Efficiency

With a melt flow index of 25 g/10 min, it fills complex molds effortlessly. Reduces cycle times and energy costs while minimizing defects in thin-walled parts.

Weather-Resistant Durability

UL-certified for outdoor use, it withstands UV exposure and temperature swings. Non-transparent properties prevent degradation, ideal for long-lasting outdoor equipment.

TAIRILITE PC Resin AC3630 Particle

Application

Household appliances

Flame-retardant housings for heaters/irons.

3C electronics

Laptop casings and power adapters.

Outdoor equipment

UV-resistant drone/controller shells.

E-bike battery cases

Impact protection for lithium packs.

Energy storage

Robust enclosures for solar battery systems.

TAIRILITE PC Resin AC3630 application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top