FCFC Plastics TAIRILITE PC Resin

TAIRILAC® AC3853 PC Resin Transparent Flame Retardant Grade

TAIRILITE AC3853 is a premium transparent flame-retardant PC resin engineered by FCFC Plastics. Combining halogen-free safety, UV resistance, and mid-low flow properties, this versatile FCFC PC resin delivers exceptional clarity and reliability for high-safety applications. Ideal for demanding industries requiring both visibility and fire protection.

  • Character: Transparency, Flame retardant, Mid-low flow, UV resistance, Halogen free.
  • Application: Transparent flame-retardant injection parts.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ISO)

  • Melt Flow Index: 12 g/10 min (ISO 1133, 300°C)
  • Impact Strength: 75 kJ/m² (Charpy, notched, ISO 179)
  • Heat Resistance: 128°C HDT (ISO 75/A, 1.8 MPa)
  • Tensile: 70 MPa | Flexural: 108 MPa (ISO 527/178)
  • Flame Rating: UL 94 V-0 (2.5mm & 3.0mm)
  • Outdoor Durability: f1-rated (UL 746C)
  • Molding Shrinkage: 0.5–0.7%

Features & Benefits

V-0 Flame Retardancy

UL 94 V-0 certified at 2.5mm/3.0mm thickness, ensuring superior fire safety without toxic halogens. Protects critical components in electrical/electronic environments.

UV-Resistant Transparency

It withstands outdoor exposure (UL 746C f1-rated), maintaining optical clarity under sunlight. Perfect for transparent covers, lenses, and displays prone to yellowing.

Halogen-Free Safety

Eco-friendly formulation eliminates toxic fumes during combustion. Safeguards user health and meets strict environmental regulations.

TAIRILITE PC Resin AC3853 Particles

Application

Electrical

Circuit breaker covers, meter housings.

Transportation

Aircraft/EV interior panels, charging station components.

Safety Gear

Visors, protective shields, emergency lighting covers.

Consumer Tech

Transparent printer housings, smart device casings.

TAIRILITE PC Resin AC3853 application

Get to Know Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top