FCFC Formosa TAIRILITE® AC3832

FCFC Plastics TAIRILITE PC Resin

TAIRILAC® AC3832 PC Resin Transparent Flame Retardant Grade

TAIRILITE AC3832 is a transparent, halogen-free PC resin offering V-0 flame retardancy, exceptional UV resistance, and low melt flow for precision molding. Ideal for demanding electrical/electronic applications, it combines safety, durability, and optical clarity.

  • Character: Transparency, Flame retardant, Low flow, UV resistance, Halogen free.
  • Application: Transparent flame-retardant sheet and injection parts.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ISO)

  • Melt Flow Index: 5 g/10 min
  • Charpy Impact Strength: 70 kJ/m² (23°C, notched)
  • Tensile Strength: 70 MPa
  • Flexural Strength: 108 MPa
  • Heat Deflection Temp: 128°C (1.8 MPa)
  • Flammability V-0 (1.0mm), 5VA (3mm): UL 94
  • Outdoor Suitability: f1 (UV/water resistant) UL 746C
  • Specific Gravity: 1.20

Features & Benefits

Uncompromised Fire Safety

It achieves UL 94 V-0 (1.0–3.0mm) and 5VA (3.0mm) ratings. Ideal for flame-retardant components without toxic halogens, meeting strict regulatory standards.

Weather-Resistant Clarity

It withstands UV/water exposure (UL f1 rating). Maintains transparency and impact strength outdoors—perfect for stadium lighting covers or traffic barriers.

Reliable Engineering Performance

It boasts 130°C RTI (electrical/mechanical) and 70 kJ/m² Charpy impact strength. Ensures long-term stability in high-heat environments like EV charging ports.

TAIRILITE PC Resin AC3832 Particles

Application

Transparent safety shields

Machine guards, riot helmets.

Flame-retardant housings

EV battery covers, server enclosures.

UV-stable components

Outdoor sensors, stadium light diffusers.

Electrical insulators

Circuit breakers, charging connectors.

TAIRILITE PC Resin AC3832 application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top