FCFC Formosa TAIRILITE® AC3873

FCFC Plastics TAIRILITE PC Resin

TAIRILAC® AC3873 Transparent Flame Retardant Grade

TAIRILITE AC3873 is a premium transparent flame-retardant PC resin engineered for demanding applications. Combining exceptional optical clarity (87%+ transmittance), inherent UV resistance, halogen-free safety, and reliable V-0 flame retardancy, it solves critical challenges in electronics, automotive, and construction components. Its low-flow properties ensure precise molding of intricate parts.

  • Character: Transparency, Flame retardant, Low flow, UV resistance, Halogen free.
  • Application: Transparent flame-retardant sheet and injection parts.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 5 g/10 min (300°C, 1.2 kg)
  • Impact Strength: 70 kJ/m² (Charpy, notched)
  • Tensile Strength: 70 MPa
  • Flexural Strength: 108 MPa
  • Heat Resistance: 128°C (HDT @1.8 MPa)
  • Optical Clarity: >87% transmission, <1.0% haze
  • Flame Rating: UL94 V-0 (1.5mm); RTI 130°C
  • Processing Dry: 4–8 hrs @120°C;
  • Processing Barrel temp 250–320°C

Features & Benefits

Flame Retardant & Safe

TAIRILITE® AC3873 achieves UL94 V-0 (1.5mm) certification without halogens, ensuring fire safety in high-risk environments like electrical housings. Ideal for eco-conscious designs.

Crystal-Clear Durability

With >87% light transmission and <1.0% haze, this PC resin maintains optical clarity while resisting UV degradation—perfect for outdoor displays or transparent protective barriers.

Process-Ready Stability

Low melt flow (5g/10min) enables controlled injection molding. Pre-drying at 120°C prevents silver streaks, ensuring consistent part quality even in complex geometries.

TAIRILITE PC Resin AC3873 Particles

Application

Transparent Flame-Retardant Sheets

Machine guards, safety windows.

Injection-Molded Electrical Parts

Connectors, circuit breakers.

UV-Exposed Components

Outdoor lighting, automotive lenses.

Consumer Electronics

Transparent covers for displays/IoT devices.

TAIRILITE PC Resin AC3873 application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top