FCFC Formosa TAIRILITE® AC2854

FCFC Plastics TAIRILITE PC Resin

TAIRILAC® AC2854 PC Resin Diffusion Grade

TAIRILITE AC2854 is a versatile polycarbonate resin engineered for superior light diffusion, balanced flow, and UV resistance. Ideal for precision-molded components requiring optical clarity and durability, it delivers consistent performance in demanding applications like LED lighting and diffusion panels.

  • Character: Light diffusion, Mid flow, UV resistance
  • Application: Diffusion board, Diffusion lamp (LED tube shell)
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Impact Strength: 70 kJ/m² (Notched Charpy, 23°C)
  • Thermal Stability: HDT 128°C (1.8 MPa)
  • Optical Clarity: Transmission 80–85% | Haze 88–91% (3.2mm)
  • Tensile: 70 MPa
  • Flexural: 108 MPa | Modulus: 2,155 MPa
  • Flammability: UL94 V-2 (0.75–3.0mm thickness)
  • RTI Electrical: 130°C | RTI Mechanical: 125°C
  • CTI: PLC 3 (High Voltage Arc Resistance)
  • Processing Temp: ≤320°C; Pre-dry: 120°C × 4–8 hrs

Features & Benefits

Built-in Light Diffusion

TAIRILITE AC2854’s optimized haze (88–91%) ensures uniform light distribution, eliminating hotspots in LED fixtures. This reduces secondary processing and enhances visual comfort.

Processing Efficiency

With mid-flow properties (MFI: 12 g/10min), it fills complex molds rapidly, cuts cycle times, and minimizes waste—ideal for high-volume production like lamp housings.

UV Defense for Longevity

UL-certified UV resistance (f1 rating) prevents yellowing and brittleness in outdoor or high-exposure environments, extending product lifespan by 3–5 years.

TAIRILITE PC Resin AC2854 Particles

Application

LED Diffusion Boards

Uniform brightness for panels & signage.

LED Tube Shells

UV-stable, impact-resistant housings.

Outdoor Lighting

F1-rated for UV/weather resistance.

Consumer Electronics

Diffusers for displays & touchscreens.

TAIRILITE PC Resin AC2854 application

Get to Know Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top