FCFC Formosa TAIRILITE® AC9140

FCFC Plastics TAIRILITE PC Resin

TAIRILAC® AC9140 PC Resin Ultra-low Temp Resistance Copolymer

TAIRILITE AC9140 is FORMOSA PC’s premium polycarbonate resin. Combining exceptional transparency (>87% transmission), mid-flow processability, and outstanding low-temperature impact resistance, this UV-stabilized material ensures reliability in high-performance 3C electronics and protective equipment. Ideal for buyers prioritizing durability and optical clarity.

  • Character: Transparency, Mid flow, Low temperature impact property, UV resistance
  • Application: Mobile phone / tablet / laptop / 3C products case, sports equipment / protective gear.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 13 g/10 min (ISO 1133)
  • Charpy Impact: 60 kJ/m² (23°C, notched) (ISO 179)
  • Heat Deflection Temp: 120°C (1.8 MPa) (ISO 75/A)
  • Tensile Strength: 60 MPa (ISO 527)
  • Flammability: UL94 V-2 (2.0mm) (IEC 60695-11-10)
  • Specific Gravity: 1.18 (ISO 1183)

Features & Benefits

Crystal-Clear Durability

TAIRILITE® PC Resin delivers >87% light transmission and <1.0% haze (ISO 13468/1), rivaling glass without brittleness. Perfect for scratch-resistant device screens and lenses.

Unmatched Impact Resilience

It withstands harsh environments (60 kJ/m² Charpy impact at 23°C, ISO 179), preventing brittle failures in sports gear or outdoor electronics in sub-zero conditions.

Safe & Stable Processing

UL-certified (RTI 80°C) and non-hazardous (SDS), it resists degradation below 320°C. Mid-flow MFI (13g/10min, ISO 1133) enables efficient molding of complex parts.

TAIRILITE PC Resin AC9140 Particles

Application

3C Electronics

Smartphone/tablet cases, laptop housings, wearables.

Protective Gear

Safety goggles, helmets, sports equipment.

Transparent Components

LED covers, medical device housings.

TAIRILITE PC Resin AC9140 application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top