FCFC Formosa TAIRILITE® AC9830

FCFC Plastics TAIRILITE PC Resin

TAIRILAC® AC9830 PC Resin Ultra-low Temp Resistance Copolymer

FCFC PC resin TAIRILITE AC9830 is an ultra-low-temperature-resistant polycarbonate copolymer. It combines translucency, mid-flow processability, UL94 V0 flame retardancy, outstanding low-temperature impact strength, and UV resistance—ideal for precision electrical and outdoor components.

  • Character: Transparency, Mid flow, Low temperature impact property, UV resistance
  • Application: Mobile phone / tablet / laptop / 3C products case, sports equipment / protective gear.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ISO)

  • Tensile Strength: 67 MPa | Flexural Strength: 98 MPa
  • Flexural Modulus: 2,058 MPa | Rockwell Hardness: R-120
  • HDT (1.8 MPa): 125°C | Autoignition Temp: >550°C
  • UL RTI (Elec/Imp/Str): 80°C (all thicknesses)
  • UL94 Rating: V-0 (1.5mm), 5VA (3.0mm) | Glow Wire (3mm): 960°C
  • Melt Flow Index: 12 g/10 min (300°C/1.2kg) | Density: 1.20 g/cm³
  • Molding Shrinkage: 0.4–0.8%

Features & Benefits

Superior Flame Retardancy

TAIRILITE AC9830 achieves UL94 V-0 (1.5mm) and 5VA (3.0mm) ratings, meeting strict safety standards. Ideal for electronics and battery housings, it reduces ignition risks without toxic additives.

Extreme Impact Resilience

With 70 kJ/m² Charpy impact strength (ISO 179, -30°C), it withstands harsh environments and physical stress. Perfect for outdoor equipment and automotive parts exposed to sub-zero temperatures.


Hassle-Free Processing

Mid-flow properties enable smooth injection molding (260–310°C barrel temp). Pre-drying (120°C, 4–8 hrs) prevents silver streaks, while UV resistance ensures long-term color stability outdoors.

TAIRILITE PC Resin AC9830 Particles

Application

Mobile/IT Equipment

Flame-retardant housings for laptops, power banks.

Electrical Components

Connectors, switches (UL RTI 80°C certified).

Outdoor Gear

UV-resistant automotive/industrial covers.

Battery Systems

UV-resistant automotive/industrial covers.

Thin-Wall Parts

0.75mm V-1 rated micro-components.

TAIRILITE PC Resin AC9830 application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top