FCFC Formosa TAIRILITE® AC2916

FCFC Plastics TAIRILITE PC Resin

TAIRILAC® AC2916 PC Resin High Transparency Grade

Tairilite AC2916 is a premium-grade polycarbonate resin engineered for high transparency and exceptional flow properties. Ideal for precision injection molding, TAIRILITE PC RESIN delivers outstanding optical clarity (>90% transmission) and process efficiency, making it perfect for demanding applications like automotive lighting and optical components.

  • Character: High Transparency, High flow
  • Application: Light guide bar, Daytime running lights for car lamp, LED condenser lens.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: Melt Flow Index: 35 g/10 min (ISO 1133, 300°C/1.2kg)
  • Tensile: 65 MPa
  • Flexural: 118 MPa
  • Flexural Modulus: 2,350 MPa
  • Impact: 55 kJ/m² (Charpy, notched)
  • Heat Resistance: 126°C (HDT @1.8 MPa)
  • Optics Transmission: >90%
  • Optics Haze: <0.5% (3.2mm thickness)
  • Safety: UL94 V-2 flammability rating (1.0–3.0mm) | RTI 80°C
  • Molding Shrinkage: 0.5–0.7%

Features & Benefits

Crystal-Clear Optical Performance

With >90% light transmission and <0.5% haze, AC2916 ensures distortion-free visibility for lenses and light guides, enhancing product aesthetics and functionality in lighting systems.

Effortless High-Flow Molding

A melt flow index of 35 g/10 min (300°C/1.2kg) enables smooth filling of intricate molds, reducing cycle times and production costs for complex parts like thin-walled lamp housings.


Reliable Impact & Heat Resistance

Boasting 55 kJ/m² Charpy impact strength and 126°C heat deflection temperature, this resin withstands mechanical stress and thermal loads in automotive and LED applications.

TAIRILITE PC Resin AC2916 Particles

Application

Light guide bars

for uniform illumination.

Daytime running lights (DRL)

in automotive lamps.

LED condenser lenses

requiring clarity and thermal stability.

TAIRILITE PC Resin AC2916 application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top