FCFC Formosa TAIRILITE® AC2955

FCFC Plastics TAIRILITE PC Resin

TAIRILAC® AC2955 PC Resin IR Transmittance Grade

FCFC PC resin Tairilite AC2955 is a mid-high flow, infrared-transparent polycarbonate engineered for precision molding. Ideal for IR-sensitive electronics, it combines exceptional optical clarity with robust processability—perfect for thin-walled components requiring reliable signal transmission.

  • Character: IR transmittance, Mid-high flow
  • Application: Applications in Information transfer, such as remote control, mobile phone PDA and wireless keyboard ect
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 20 g/10 min (300°C, 1.2 kg)
  • Impact Strength: 65 kJ/m² (Charpy, notched)
  • Heat Resistance: 128°C (HDT @1.8 MPa)
  • Flexural Strength: 110 MPa | Flexural Modulus: 2,205 MPa
  • Tensile Strength: 68 MPa
  • Shrinkage Rate: 0.5–0.7%
  • Flammability: UL94 V-2 (1.0–3.0mm, all colors)
  • Specific Gravity: 1.2

Features & Benefits

Infrared Signal Transparency

It enables flawless IR transmission (e.g., remote controls, sensors), ensuring uninterrupted data transfer without compromising structural integrity.

Mid-High Flow Efficiency

Accelerates production cycles for complex geometries (e.g., slim keyboard casings), reducing energy use and minimizing sink marks.


Reliable Flame Resistance

UL94 V-2 certified at 1.0–3.0mm thickness, safeguarding electronics against combustion risks in compact designs.

TAIRILITE PC Resin AC2955 Particles

Application

Consumer Electronics

Remote controls, wireless keyboards, VR headsets.

Mobile Devices

Smartphone/PDA sensor housings, IR blasters.

IoT Hardware

Wearable health monitors, optical communication modules.

TAIRILITE PC Resin AC2955 application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity