FCFC Formosa TAIRILITE® AC3600-AF

FCFC Plastics TAIRILITE PC Resin

TAIRILAC® AC3600-AF PC Resin Self Extinguishing Grade

TAIRILITE PC Resin AC3600-AF is a high-flow, non-transparent polycarbonate raw material. This halogen-free (Cl/Br/Sb-free), flame-retardant material delivers exceptional impact resistance and thermal stability, ideal for precision-molded components requiring safety compliance and reliability.

  • Character: High flow, Non-transparency, Cl, Br, Sb free, Flame retardant
  • Application: Transformer case, Battery case, Projector housing, Electroomechanical appliance cover
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 10 g/10 min (300°C, 1.2 kg)
  • Impact Strength: 735 J/m (23°C)
  • Heat Resistance: 113°C HDT (1.8 MPa)
  • Flexural Strength: 99 MPa | Flexural Modulus: 2,150 MPa
  • Tensile Strength: 67 MPa
  • Molding Shrinkage: 0.5–0.7%
  • Flame Rating: UL94 V-0 (1–3 mm), V-1 (0.8 mm), V-2 (0.6 mm)
  • Specific Gravity: 1.19
  • Pre-Drying: 110–120°C × 4–6 hrs
  • Screw Temp: 260–295°C
  • Injection Pressure: 50–130 kg/cm²
  • Mold Temp: 80–100°C

Features & Benefits

Halogen-Free Flame Retardancy

AC3600-AF achieves UL94 V-0 fire resistance (1–3 mm thickness) without toxic halogens or antimony. Ensures safety in electrical components while meeting eco-friendly regulations.

Superior Impact Resistance

With 735 J/m Izod impact strength (ISO 180), it withstands drops and shocks in rugged environments, reducing part failures in automotive or industrial housings.

High-Flow Processing Efficiency

Melt flow index of 10 g/10 min (ISO 1133) enables easy filling of intricate molds, cutting cycle times and production costs for complex geometries.

TAIRILITE PC Resin AC3600-AF Particles

Application

Transformer Cases

Flame-retardant protection for electrical insulation.

Battery Enclosures

Impact-resistant safety for EV/power storage systems.

Projector Housings

Precision molding for complex optical equipment.

Electromechanical Covers

Durability in industrial machinery and IoT devices.

TAIRILITE PC Resin AC3600-AF application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top