TAIRIPRO® K1035 PP Resin Injection Molding
TAIRIPRO K1035 is a high-performance polypropylene homopolymer resin designed for injection molding. With high fluidity, excellent stiffness, and superior surface luster, this PP K1035 resin streamlines production while delivering durable, visually appealing results for thin-walled parts, housewares, and toys.
Basic Features:
- Manufacturer: FCFC (Formosa Chemicals & Fibre Corporation)
- Character: High fluidity, Good Stiffness, Good luster
Key technical data (ISO)
- Melt Flow Index: 38 g/10 min (ISO 1133)
- Heat Resistance: 110°C HDT
- Safety Compliance: UL 94 HB flammability rating
- Molding Shrinkage: 1.4–1.8%

Applications
- Thin-Wall Parts: Food packaging, disposable cups, and medical containers
- Housewares: Durable storage boxes, kitchen utensils, and appliance components
- Toys: Intricate action figures, snap-fit components, and outdoor playsets

Tairipro® K1035 Datasheet
| Injection Molding Grade FCFC TAIRIPRO® K1035 Data Sheet | ||||
| Product Description: High fluidity, Good Stiffness, Good luster | ||||
| Property | Unit | Test Method | Test Condition | Model K1035 |
| Melt Flow Index | g/10 min | ISO 1133 | 230℃ × 2.16kg | 38 |
| IZOD Impact Strength | kJ/m² | ISO 180 | 23℃,1/8″,Notched | 2 |
| IZOD Impact Strength | kJ/m² | ISO 180 | 23℃,4mm,Notched | 2 |
| Specific Gravity | – | ISO 1183 | 23℃/23℃ | 0.9 |
| Tensile Strength | Mpa | ISO 527 | 23℃,50mm/min | 33 |
| Tensile Elongation at break | % | ISO 527 | 23℃,50mm/min | >50 |
| Flexural Modulus | Mpa | ISO 178 | 23℃ | 14000 |
| Rockwell Hardness | R-scale | ISO 2039-2 | 23℃ | R-102 |
| Heat Deflection Temperature | ℃ | ISO 75/A | Unannealed,0.455Mpa 1/4″ thickness,120℃/h | 110 |
| Molding Shrinkage | % | FCFC Method | 23℃ | 1.4 ~ 1.8 |
| Combustibility | UL-94 | File No. E162823 | HB 1.5 mm | |
| All tests were run under laboratory conditions, ASTM, ISO testing procedures. | ||||
| The data are intended as a general guide only. | ||||
| Formosa Chemicals & Fibre Corp. Plastics Div. | ||||
Tairipro® K1035 UL Product iQ
| TAIRIPRO® K1035 UL Product iQ | ||
| File Number: E162823 | Polypropylene (PP), pellets | |
| Flammability | Value | Test Method |
| Flame Rating | ||
| 1.5 mm, ALL | HB | UL 94 |
| 1.5 mm, ALL | HB75 | IEC 60695-11-10, -20 |
| Electrical | Value | Test Method |
| Hot-wire Ignition (HWI) (1.5 mm) | PLC 3 | UL 746 |
| High Amp Arc Ignition (HAI) (1.5 mm) | PLC 3 | UL 746 |
| Comparative Tracking Index (CTI) | PLC 0 | UL 746 |
| High Voltage Arc Tracking Rate (HVTR) | PLC 0 | UL 746 |
| Arc Resistance | PLC 4 | ASTM D495 |
| Thermal | Value | Test Method |
| RTI Elec | UL 746 | |
| 1.5 mm | 65.0°C | |
| 3.0 mm | 65.0°C | |
| RTI Imp | UL 746 | |
| 1.5 mm | 65.0°C | |
| 3.0 mm | 65.0°C | |
| RTI Str | UL 746 | |
| 1.5 mm | 65.0°C | |
| 3.0 mm | 65.0°C | |
Related Tairipro® PP Plastics
FCFC TAIRIPRO® K1011 PP Resin
FCFC Formosa TAIRIPRO® K9010
FCFC TAIRIPRO® K2051 PP Resin
FCFC TAIRIPRO® B1101 PP Resin
FCFC Formosa TAIRIPRO® K7009
FCFC Formosa TAIRIPRO® K8025
FCFC Formosa TAIRIPRO® K9030
FCFC TAIRIPRO® S1005 PP Resin
FCFC Formosa TAIRIPRO® B8001
FCFC TAIRIPRO® K4535 PP Resin
FCFC TAIRIPRO® T1202 PP Resin
FCFC Formosa TAIRIPRO® K7005AG
FCFC Formosa TAIRIPRO® F4007
FCFC Formosa TAIRIPRO® B8001A3
FCFC Formosa TAIRIPRO® K8009
FCFC Formosa TAIRIPRO® K8802
FCFC Formosa TAIRIPRO® K3029
FCFC TAIRIPRO® F2011 PP Resin
Advanced Manufacturing