FCFC TAIRILAC® AG15A1-H ABS

Formosa Plastics TAIRILAC AG15A1-H

TAIRILAC® AG15A1-H ABS Resin General Grade

TAIRILAC AG15A1-H ABS Resin (by Formosa) is a high-gloss, medium-impact plastic perfect for toys, phone cases, luggage, and electronics. It handles heat up to 94°C, stays strong under stress (45MPa tensile, 68MPa flexural), and molds smoothly with low shrinkage (0.4–0.7%). The HB flammability rating ensures safety for household items. Durable, heat-resistant, and easy to shape—ideal for sleek, reliable designs.

  • Character: High gloss, Medium impact
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 21 g/10 min (220°C/10kg) | Specific Gravity: 1.05 (lightweight)
  • Heat Resistance: Vicat Softening Point @94°C | HDT @90°C (1.8MPa)
  • Mechanical Strength: Tensile Strength @45 MPa | Flexural Strength @68 MPa
  • Molding Shrinkage: 0.4–0.7% (consistent dimensional stability)

Balanced Durability & Safety

UL94 HB flammability rating (1–3mm) and medium impact strength protect products like suitcases or toys from damage and meet basic fire safety standards.

Smooth Molding Efficiency

With a melt flow index of 21 g/10 min (220°C/10kg), Tairilac ABS AG15A1-H fills molds quickly, reducing cycle times for thin-walled parts like calculator casings or phone housings.

Aesthetic Surface Finish

High gloss and Rockwell hardness R-110 ensure scratch-resistant, premium surfaces—ideal for stereo housings or clock faces demanding visual appeal.

Formosa Plastics TAIRILAC® AG15A1-H ABS Resin

Application

  • Toys: Medium impact strength withstands drops, while high gloss retains vibrant colors.
  • Phone/Stereo Housings: Scratch-resistant surfaces stay pristine through daily use.
  • Calculators/Clocks: Smooth molding ensures crisp edges and flawless finishes.
  • Suitcases: Lightweight yet tough construction resists cracks during travel.
Formosa Plastics TAIRILAC AG15A1-H application

Tairilac® AG15A1-H Datasheet

General grade FCFC TAIRILAC® AG15A1-H Data Sheet
Product Description: High gloss, Medium impact
PropertyUnitTest MethodTest ConditionGeneral Grade
Melt Flow Indexg/10 minISO 1133200℃ × 5kg2.2
Melt Flow Indexg/10 minISO 1133220℃ × 10kg21
Specific GravityISO 118323℃/23℃1.05
Tensile StrengthMpaISO 52723℃, 50mm/min45
Flexural StrengthMpaISO 17823℃, 2mm/min68
Flexural ModulusMpaISO 17823℃, 2mm/min2400
Rockwell HardnessR-scaleISO 2039-223℃R-110
Vicat Softening PointISO 306Annealed, 50N,50℃/h94
Heat Deflection TemperatureISO 75/AAnnealed, 1.8Mpa 4mm thick,120℃/h90
Molding Shrinkage%ISO 25773.2mm0.4 ~ 0.7
CombustibilityUL-94File No. E162823HB 1 ~ 3 mm

Tairilac® AG15A1-H UL Product iQ

TAIRILAC® ANC160 UL Product iQ
File Number: E162823Acrylonitrile Butadiene Styrene (ABS), pellets
FlammabilityValueTest Method
Flame Rating
1.0 mm, ALLHBUL 94
1.5 mm, ALLHBUL 94
3.0 mm, ALLHBUL 94
3.0 mm, ALLHB40IEC 60695-11-10, -20
1.0 mm, ALLHB75IEC 60695-11-10, -20
1.5 mm, ALLHB75IEC 60695-11-10, -20
ElectricalValueTest Method
Hot-wire Ignition (HWI)UL 746
1.0 mmPLC 4
1.5 mmPLC 4
3.0 mmPLC 3
High Amp Arc Ignition (HAI)UL 746
1.0 mmPLC 0
1.5 mmPLC 0
3.0 mmPLC 0
Comparative Tracking Index (CTI)PLC 0UL 746
High Voltage Arc Tracking Rate (HVTR)PLC 2UL 746
Arc ResistancePLC 6ASTM D495
ThermalValueTest Method
RTI ElecUL 746
1.0 mm60.0°C
1.5 mm75.0°C
3.0 mm95.0°C
RTI ImpUL 746
1.0 mm60.0°C
1.5 mm60.0°C
3.0 mm80.0°C
RTI StrUL 746
1.0 mm60.0°C
1.5 mm60.0°C
3.0 mm95.0°C

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top