FCFC TAIRILAC® ANC160 ABS

Formosa Plastics TAIRILAC ANC160

TAIRILAC® ANC160 ABS Self Extinguishing Grade

TAIRILAC ANC160 by Formosa Plastics is a flame retardant ABS resin. It’s great for making parts of electronic devices like LCD monitors and computers because it doesn’t catch fire easily. It has the best flame retardancy rating, stopping burning quickly. It’s also good with electricity and can handle heat up to 60°C without problems.

  • Manufacturer: Formosa Plastics (FCFC)
  • Character: Flame retardant
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Flame Retardancy: UL 94 V-0 (2.5mm & 3.0mm) | IEC 60695-11-10 certified.
  • Electrical Safety: Hot-Wire Ignition (HWI): PLC 2 (resists ignition); Arc Resistance: PLC 6 (excellent for high-voltage parts).
  • Thermal Performance: RTI (Electrical/Mechanical/Impact): 60°C across all metrics.
  • Heat Resistance: Vicat Softening Point @120°C
  • Compliance: UL 746, ASTM D495, and IEC standards

UL 94 V-0 Flame Retardancy

TAIRILAC ABS ANC160 meets stringent UL 94 V-0 standards (2.5–3.0mm), ensuring self-extinguishing properties. Ideal for reducing fire risks in electronics and high-heat environments.

Reliable Electrical Performance

It resists sparks and short circuits (HAI PLC 0, HWI PLC 2). This material handles electricity well, with top scores in arc and tracking tests, perfect for electronics.

Thermal Stability Under Stress

A RTI of 60°C ensures dimensional stability in heat-intensive applications, prolonging product lifespan for devices like LCD-TV housings and power units.

Formosa Plastics TAIRILAC® ANC160 ABS Resin

Application

  • Office Equipment Housings: TAIRILAC ANC160’s flame retardancy and PLC 0 HAI rating make it ideal for printers and copiers, preventing electrical fires in busy office environments.
  • Consumer Electronics: Used in LCD monitor and TV casings, ANC160’s UL 94 V-0 rating ensures compliance with global safety standards while resisting heat from prolonged use.
  • Industrial Machinery Components: Its thermal stability (RTI 60°C) and arc resistance suit high-amp industrial devices, reducing maintenance costs and downtime.
Formosa Plastics TAIRILAC ANC160 application

Tairilac® ANC160 Datasheet

Self Extinguishing Grade FCFC TAIRILAC® ANC160 Data Sheet
Product Description: Flame retardant
PropertyUnitTest MethodTest ConditionModel ANC160
CombustibilityUL-94File No. E162823v-0 2.5 mm

Tairilac® ANC160 UL Product iQ

TAIRILAC® ANC160 UL Product iQ
File Number: E162823Acrylonitrile Butadiene Styrene (ABS), pellets
FlammabilityValueTest Method
Flame RatingUL 94
2.5 mm, ALLV-0IEC 60695-11-10, -20
3.0 mm, ALLV-0
ElectricalValueTest Method
Hot-wire Ignition (HWI)UL 746
2.5 mmPLC 2
3.0 mmPLC 2
High Amp Arc Ignition (HAI)UL 746
2.5 mmPLC 0
3.0 mmPLC 0
Comparative Tracking Index (CTI)PLC 0UL 746
High Voltage Arc Tracking Rate (HVTR)PLC 0UL 746
Arc ResistancePLC 6ASTM D495
ThermalValueTest Method
RTI ElecUL 746
2.5 mm60.0°C
3.0 mm60.0°C
RTI ImpUL 746
2.5 mm60.0°C
3.0 mm60.0°C
RTI StrUL 746
2.5 mm60.0°C
3.0 mm60.0°C

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top