Formosa TAIRILAC® AG12A0 ABS

Formosa Plastics TAIRILAC ANC160

TAIRILAC® AG12A0 ABS Resin General Purpose Grade

Tairilac AG12A0 is a super high-impact ABS resin engineered for toughness and process efficiency. Ideal for injection molding and extrusion in demanding industrial applications, combining durability with safety compliance.

  • Manufacturer: Formosa Plastics (FCFC)
  • Character: Super high impact
  • Application: Helmets, Shoe heels, Pipe fittings, Products of low-temp usage
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ISO)

  • Impact Strength: 30 kJ/m² (ISO 179, notched)
  • Melt Flow: 19 g/10min (220°C/10kg, ISO 1133)
  • Tensile Strength: 44 MPa (ISO 527)
  • Vicat Softening: 93°C (ISO 306)
  • HDT (1.8 MPa): 94°C (ISO 75)
  • Flammability: UL94 HB (1.5–3.0 mm)
  • Shrinkage: 0.4–0.7%
  • Specific Gravity: 1.04

Features & Benefits

Extreme Impact Resistance

Charpy impact strength of 30 kJ/m² ensures reliability in high-stress environments, reducing part failures and replacements.

Optimized Processing

Low pre-drying (70–80°C, 2–3 hrs) and versatile molding temps (190–230°C) cut energy costs and cycle times.

Safety-Certified

UL94 HB flammability rating and RTI 60°C electrical safety meet strict standards without additives.

FCFC Formosa TAIRILAC ABS Resin

Application

Protective Helmets

Industrial Shoe Heels

Pressure-Resistant Pipe Fittings

Low-Temperature Components

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top