Formosa TAIRILAC® AF3500 ABS

Formosa Plastics TAIRILAC ANC160

TAIRILAC® AF3500 ABS Resin High Flow Grade

Tairilac® AF3500 ABS resin by Formosa ABS producers combines exceptional flow properties with robust impact resistance, ideal for intricate thin-walled designs. This versatile grade streamlines injection molding while ensuring durability in high-stress environments.

  • Manufacturer: Formosa Plastics (FCFC)
  • Character: High flow, High impact
  • Application: Housing of stereos, Large toys, Chairs, Motorcycles, OA machines
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Rate (220°C): 47 g/10 min (ISO 1133)
  • Charpy Impact Strength: 31 kJ/m² (notched, 23°C) (ISO 179)
  • Tensile Strength: 38 MPa (≈387 kg/cm²) (ISO 527)
  • Flexural Modulus: 1,500 MPa (ISO 178)
  • HDT (Annealed, 1.8 MPa): 90°C (ISO 75/A)
  • Flammability Rating: HB (UL 94, 1.5–3.0 mm) (UL 94)

Features & Benefits

Superior Flow for Complex Molds

With an ultra-high melt flow index (ISO 1133: 47 g/10min at 220°C/10kg), AF3500 fills intricate geometries effortlessly, reducing cycle times and injection pressure by up to 15%.

High Impact Resilience

Delivering 31 kJ/m² Charpy impact strength (ISO 179), it withstands drops and impacts in rugged applications like automotive trims and outdoor equipment without cracking.

Balanced Processing Stability

It pre-dries at just 70–80°C (2–3 hrs), features low mold shrinkage (0.4–0.7%), and processes smoothly at 180–230°C screw temps—minimizing warpage and energy costs.

FCFC Formosa TAIRILAC ABS Resin

Application

Electronics

Stereo housings, printer casings (UL HB rating ensures safety).

Consumer Goods

Large toy parts, garden chairs (impact-resistant for rough use).

Transportation

Motorcycle fairings, helmet shells (balances lightness and toughness).

Industrial

Office automation (OA) machine covers (high flow for sleek finishes).

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top