Formosa TAIRILAC® AX4000

Formosa Plastics TAIRILAC ANC160

TAIRILAC® AX4000 ABS Resin Heat Resistant Grade

Tairilac® AX4000 ABS Resin is a medium-high heat-resistant thermoplastic. Delivering exceptional thermal stability and mechanical strength, it excels in components exposed to elevated temperatures while maintaining easy processability for injection molding.

  • Manufacturer: Formosa Plastics (FCFC)
  • Character: Medium high heat
  • Application: Parts of cars, Electrical appliances, Hair dryer, Heat resistant parts
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Melt Flow Index: 9 g/10 min (220°C, 10 kg)
  • Charpy Impact: 21 kJ/m² (23°C, notched)
  • Tensile Strength: 41 MPa
  • Flexural Strength: 63 MPa | Flexural Modulus: 2,100 MPa
  • Heat Deflection Temp. (HDT): 96°C (1.8 MPa, annealed)
  • Molding Shrinkage: 0.3–0.6% (3.2 mm thickness)
  • Flammability: UL 94 HB (1.5 mm)
  • Rockwell Hardness: R-109
  • Specific Gravity: 1.05

Features & Benefits

Enhanced Heat Resistance

With a Vicat softening point of 100°C and heat deflection temperature (HDT) of 96°C (ISO 75/A), Tairilac ABS AX4000 withstands high-heat environments without deformation—ideal for automotive under-hood parts and electrical housings.

Superior Impact Strength

Boasting 21 kJ/m² Charpy impact resistance (ISO 179), this grade absorbs shocks and stresses in appliances like power tools or automotive trim, reducing failure risks in high-vibration scenarios.

Optimized Processing Ease

It pre-dries quickly at 90–95°C (2–3 hrs) and processes smoothly at 200–250°C screw temperatures, minimizing cycle times and energy costs for complex geometries like hair dryer nozzles.

FCFC Formosa TAIRILAC ABS Resin

Application

Automotive

Engine bay components, dashboards, and vents.

Electrical Appliances

Housings for routers, printers, and power supplies.

Personal Care

Hair dryer nozzles, straightener casings.

Industrial

Heat-resistant enclosures and structural parts.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity