Formosa TAIRILAC® AX4300 ABS

Formosa Plastics TAIRILAC ANC160

TAIRILAC® AX4300 ABS Resin Heat Resistant Grade

Formosa Plastics TAIRILAC® AX4300 ABS resin delivers exceptional heat resistance. Engineered for demanding applications, this medium-high heat grade maintains structural integrity under thermal stress while offering outstanding mechanical balance. Ideal for automotive and appliance components.

  • Manufacturer: Formosa Plastics (FCFC)
  • Character: Medium high heat, Extrusion blow molding
  • Application: Parts of cars, Electrical appliances, Hair dryer, Heat resistant parts
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 4 g/10 min, ISO 1133 (220°C/10kg)
  • Charpy Impact Strength: 28 kJ/m² (notched, 23°C) (ISO 179)
  • Tensile Strength: 42 MPa (ISO 527)
  • Flexural Strength: 62 MPa (ISO 178)
  • Flexural Modulus: 2,000 MPa (ISO 178)
  • Rockwell Hardness: R-106 (ISO 2039-2)
  • Mold Shrinkage: 0.3–0.6% (3.2mm thickness) (ISO 2577)

Features & Benefits

Enhanced Heat Resistance

With a Heat Deflection Temperature (HDT) of 96°C @ 1.8MPa (ISO 75/A) and Vicat softening point of 99°C, Tairilac ABS AX4300 withstands sustained high-temperature environments without warping, ensuring dimensional stability in heat-exposed parts.

Optimized Processing Flexibility

Pre-dry at 90–95°C for 2–3 hours and process via extrusion blow molding. Its balanced flow (Melt Flow Index: 4g/10min, ISO 1133) enables complex geometries with consistent mold shrinkage (0.3–0.6%), reducing production waste.

Robust Mechanical Properties

It combines high impact strength (28 kJ/m² Charpy, ISO 179) with rigidity (Flexural Modulus: 2,000 MPa, ISO 178) and hardness (R-106), offering durability for functional parts under mechanical stress.

FCFC Formosa TAIRILAC ABS Resin

Application

Automotive

Engine bay components, vent housings, and under-hood clips.

Appliances

Hair dryer nozzles, heater housings, and microwaveable parts.

Electrical

Heat-resistant enclosures for power tools and connectors.

Industrial

Blow-molded ducts, HVAC components, and industrial

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top