Formosa TAIRILAC® ANC100 ABS

Formosa Plastics TAIRILAC ANC160

TAIRILAC® ANC100 ABS Resin Heat Resistant Grade

Tairilac® ANC100 is a flame-retardant ABS resin engineered for high-safety applications. This self-extinguishing grade combines UL94 V-0 compliance, robust mechanical strength, and excellent processability—ideal for electronics housings and critical components

  • Manufacturer: Formosa Plastics (FCFC)
  • Character: Flame retardant
  • Application: Flame retardant materials; Housing of LCD monitor, LCD-TV, computers & OA machine
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (iSO)

  • Flow: Melt Flow Index: 6 g/10 min (200°C, 5kg)
  • Strength: Tensile: 40 MPa | Flexural: 59 MPa | Impact: 17 kJ/m² (notched)
  • Thermal: HDT (1.8MPa): 76°C | Vicat Softening: 80°C
  • Safety: UL94 V-0 (1.5–3mm) & 5VA (2.3–2.5mm) | Glow Wire Ignition: 700°C
  • Processing: Screw Temp: 160–200°C | Mold Temp: 40–70°C

Features & Benefits

Superior Flame Retardancy

Tairilac ABS ANC100 achieves UL94 V-0 (1.5–3mm) and 5VA (2.3–2.5mm) ratings, minimizing fire risks in electronics without compromising part thickness. Benefit: Enhances end-product safety for consumer-facing devices.

High Mechanical Performance

With 17 kJ/m² impact strength (ISO 179) and 40 MPa tensile strength (ISO 527), it resists cracks and deformation under stress. Benefit: Extends product lifespan in demanding environments like industrial housings.

Easy Processing & Stability

It features low mold shrinkage (0.3–0.6%, ISO 2577) and optimized drying (70–80°C × 2–3hr), enabling precision molding of complex parts. Benefit: Reduces waste and accelerates production cycles.

FCFC Formosa TAIRILAC ABS Resin

Application

Flame-retardant enclosures

LCD monitors, TVs, and computer housings.

Office automation (OA) equipment

Printers, scanners, and copier casings.

Consumer electronics

Power adapters, sockets, and IoT device shells.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top