Formosa TAIRILAC® AG10NP ABS

Formosa Plastics TAIRILAC ANC160

TAIRILAC® AG10NP ABS Resin Extrusion Grade

TAIRILAC® AG10NP ABS Resin is FCFC’s trusted extrusion-grade solution, engineered for super-high impact resistance and exceptional rigidity. Ideal for demanding applications like protective gear and industrial profiles, it delivers reliable performance with easy processing.

  • Manufacturer: Formosa Plastics (FCFC)
  • Character: Extrusion molding, Super high impact, High rigid
  • Application: Extrusion products,Crash helmets,Pipes, Shoe heels
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (iSO)

  • Melt Flow Index: 5.5 g/10 min (220°C, 10 kg)
  • Impact Strength: 45 kJ/m² (Charpy, notched)
  • Tensile Strength: 42 MPa
  • Flexural Modulus: 1,900 MPa
  • Vicat Softening: 94°C (ISO 306)
  • HDT (1.8 MPa): 93°C (ISO 75/A)
  • Flame Safety: HB Rating (UL 94, 1.6–1.76 mm)
  • Non-hazardous (GHS/US OSHA)
  • Dust explosion-resistant (ISO handling protocols)
  • UL RTI Electrical/Mechanical: 60°C

Features & Benefits

Extreme Impact Protection

With 45 kJ/m² Charpy impact strength (ISO 179), AG10NP absorbs sudden shocks without cracking – perfect for crash helmets or safety equipment exposed to drops or collisions.

Structural Rigidity Assurance

A high flexural modulus (1,900 MPa, ISO 178) ensures dimensional stability under load, preventing warping in pipes, automotive trims, or load-bearing components.

Optimized Extrusion Efficiency

It pre-dries quickly (70–80°C/2–3 hrs) and processes smoothly at 180–230°C screw temps, reducing energy use and production downtime for profiles or sheets.

FCFC Formosa TAIRILAC ABS Resin

Application

Protective Gear

Bicycle/motorcycle helmets requiring impact absorption.

Industrial Pipes

Chemical-resistant conduits needing rigidity and pressure tolerance.

Consumer Goods

Durable shoe heels resistant to repetitive stress.

Extrusion Profiles

Window seals, automotive trims, and DIY tool handles.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top