Formosa TAIRILAC® AE8700 ABS

Formosa Plastics TAIRILAC ANC160

TAIRILAC® AE8700 ABS Resin Extrusion Grade

Tairilac® AE8700 is an extrusion-grade ABS resin engineered for super high impact resistance and exceptional rigidity. Ideal for demanding industrial profiles, it delivers unmatched dimensional stability and processability in extrusion molding.

  • Manufacturer: Formosa Plastics (FCFC)
  • Character: Extrusion molding, Super high impact, High rigid
  • Application: Extrusion products,Crash helmets,Pipes, Shoe heels
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (iSO)

  • Melt Flow Index: 3.5 g/10 min (220°C, 10kg)
  • Impact Strength: 40 kJ/m² (Charpy, notched)
  • Tensile Strength: 46 MPa
  • Flexural Strength: 69 MPa | Flexural Modulus: 2300 MPa
  • Vicat Softening Point: 95°C
  • Heat Deflection Temp (annealed): 87°C (1.8 MPa)
  • Molding Shrinkage: 0.4–0.7%
  • Specific Gravity: 1.04

Features & Benefits

Extrusion-Optimized Processability

With a balanced melt flow (3.5 g/10 min), AE8700 ensures smooth, efficient extrusion – reducing energy waste and production downtime for pipes and profiles.

Impact Resistance for Safety

Unmatched Charpy impact strength (40 kJ/m²) absorbs high-force impacts, ideal for crash helmets or protective gear that must withstand harsh conditions.

Rigidity Under Pressure

High flexural modulus (2300 MPa) prevents warping in structural parts like shoe heels or load-bearing components, ensuring long-term durability.

FCFC Formosa TAIRILAC ABS Resin

Application

Extrusion Products

Consistent, warp-free profiles for window frames and industrial tubing.

Crash Helmets

Impact absorption for motorcycle/sports safety gear.

Pipes

Thermal stability and pressure resistance in fluid-transport systems.

Shoe Heels

Lightweight rigidity for durable footwear support.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity