Formosa TAIRILAC® ANC120 ABS

Formosa Plastics TAIRILAC ANC160

TAIRILAC® ANC120 ABS Resin Self Extinguishing Grade

Tairilac® ANC120 ABS Resin is a flame-retardant engineering plastic designed for high-safety applications. This UL94 V-0/5VB-certified material combines exceptional fire resistance with balanced mechanical properties, ideal for thin-walled electronics housings and office equipment.

  • Manufacturer: Formosa Plastics (FCFC)
  • Character: Flame retardant
  • Application: Flame retardant materials; Housing of LCD monitor, LCD-TVcomputers & OA machine
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (iSO)

  • Flame Rating: UL94 V-0 & 5VB (2.3–3.0 mm)
  • Impact Strength: 18 kJ/m² (Charpy, notched)
  • HDT @1.8 MPa: 79°C (ISO 75/A)
  • Vicat Softening: 83°C
  • Melt Flow: 5.5 g/10 min (200°C/5kg)
  • Mold Shrinkage: 0.3–0.6%
  • Glow Wire Ignition: 700°C (IEC 60695-2-13)
  • CTI: PLC 2 (UL 746)

Features & Benefits

Optimized Flame Resistance

ANC120 exceeds stringent safety standards (UL94 V-0/5VB at 2.3–3.0 mm thickness), reducing ignition risks in electronics. Its halogen-based formulation ensures reliable protection without compromising processability.

Energy-Efficient Processing

With low molding temperatures (160–200°C) and short drying cycles (70–80°C/2–3 hrs), ANC120 cuts energy use and speeds up production, lowering operational costs.

Balanced Mechanical Performance

The resin delivers high impact strength (18 kJ/m² ISO 179) and rigidity (2,000 MPa flexural modulus), preventing warpage in slim-profile designs like monitor bezels.

FCFC Formosa TAIRILAC ABS Resin

Application

LCD Monitor/TV Bezels

Meets slim design needs with V-0 fire resistance.

Computer & Printer Housings

Withstands impact while ensuring electrical safety.

Office Automation (OA) Equipment

Complies with international combustibility standards for power units.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer