Formosa TAIRILAC® AX4100 ABS

Formosa Plastics TAIRILAC ANC160

TAIRILAC® AX4100 ABS Resin Heat Resistant Grade

Tairilac® AX4100 is a premium heat-resistant ABS resin engineered for superior performance in high-temperature environments. Delivering exceptional thermal stability and mechanical strength, it’s ideal for automotive, electronics, and consumer appliances.

  • Manufacturer: Formosa Plastics (FCFC)
  • Character: Super high heat
  • Application: Parts of cars, Electrical appliances, Hair dryer, Heat resistant parts
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (iSO)

  • Vicat Softening Point: 106°C (ISO 306)
  • Heat Deflection Temp (1.8 MPa): 102°C (ISO 75/A)
  • Tensile Strength: 38 MPa (ISO 527)
  • Charpy Impact: 16 kJ/m² (ISO 179, notched)
  • Flexural Modulus: 2,100 MPa (ISO 178)
  • Flammability: UL 94 HB (1.5 mm thickness)
  • RTI (Electrical/Mechanical): 60°C (UL 746)
  • Molding Shrinkage: 0.3–0.6% (ISO 2577)
  • Melt Flow Index: 4.5 g/10 min (ISO 1133)

Features & Benefits

Exceptional Heat Resistance

With a Vicat softening point of 106°C and HDT up to 102–112°C, AX4100 withstands intense heat without deforming—perfect for components near engines or heating elements.

Reliable Mechanical Strength

It offers high tensile strength (38 MPa) and impact resistance (16 kJ/m²), ensuring durability in structural parts like automotive housings or appliance gears.

Safe & Easy Processing

It pre-dries at 90–95°C and processes smoothly at 200–250°C. UL 94 HB-rated for flammability safety, with low dust risks when handled properly.

FCFC Formosa TAIRILAC ABS Resin

Application

Automotive

Engine covers, HVAC components, and other under-hood parts needing heat resistance.

Electrical Appliances

Housings for routers, power tools, and connectors.

Consumer Durables

Hair dryer nozzles, coffee makers, and steam iron parts.

Industrial

Heat-resistant enclosures for machinery and sensors.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top