Formosa TAIRILAC® AG20GF ABS

Formosa Plastics TAIRILAC ANC160

TAIRILAC® AG20GF ABS Resin 20%GF Reinforced Grade

Tairilac® AG20GF by Formosa Plastics ABS is a 20% glass fiber-reinforced resin engineered for exceptional dimensional stability and high heat resistance. Perfect for precision injection-molded components demanding durability and thermal performance.

  • Manufacturer: Formosa Plastics (FCFC)
  • Character: Dimensional stability, High heat resistant
  • Application: Printer parts
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (iSO)

  • Melt Flow Index: 15 g/10 min (220°C, 10 kg)
  • Impact Strength: 8.7 kg-cm/cm (IZOD, notched)
  • Thermal Rating: RTI 60°C (Elec/Imp/Str)
  • Flammability: UL 94 HB (1.5–1.7 mm)
  • Processing: Pre-dry at 70–80°C for 2–3 hrs; mold temp 40–80°C
  • Safety: Non-hazardous (GHS compliant)

Features & Benefits

Enhanced Structural Integrity

Glass fiber reinforcement boosts tensile strength (1,100 kg/cm²) and flexural rigidity (69,510 kg/cm²), ensuring parts withstand heavy loads without deformation. Ideal for high-stress applications.

Superior Heat Resistance

It withstands temperatures up to 250°C during processing and continuous use at 60°C (RTI). Prevents warping in thermal environments like printers or automotive components.

Minimal Shrinkage & Warping

Low mold shrinkage (0.4–0.7%) guarantees precise tolerances and dimensional stability—critical for intricate parts like gears or housings.

FCFC Formosa TAIRILAC ABS Resin

Application

Printer parts

Frames, gears, and covers requiring heat resistance, dimensional precision, and structural strength to endure mechanical stress and repeated use.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity