Suke Plastics FR865C ABS Resin

Suke Plastics Modified Plastic

Suke FR865C ABS Resin Flame Retardant Grade

Suke FR865C is an eco-compliant, flame-retardant ABS resin engineered for demanding industrial applications. Passing RoHS standards with UL94 V0 certification (2.5mm), it combines safety, process efficiency, and structural reliability for electronics, printers, and office equipment.

  • Manufacturer: Suke Plastics
  • Character: Pass RoHS, Flame retardant
  • Application: printer; Electrical &electronic; Office supplies
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ASTM)

  • Density: 1.17 g/cm³
  • Mold Shrinkage: 0.4–0.7% (2mm)
  • Tensile Strength: 40 MPa
  • Flexural Strength: 67 MPa
  • Impact Strength (Notched IZOD): 18 kJ/m² (3.2mm, 23°C)
  • HDT @0.45MPa: 82°C
  • UL94 Rating: V0 (2.5mm)
  • Processing Melt Temp: 210°C (Max 230°C)
  • Processing Drying: 80°C × 3hr
  • Processing Mold Temp: 70°C

Application

  • Printers: Housings, paper trays, structural frames.
  • Electrical & Electronics: Connectors, switches, enclosures.
  • Office Supplies: Durable casings for devices, ergonomic tools.
Suke FR865C ABS plastic application
Suke FR865C ABS plastic

Features & Benefits

Safety & Compliance Guaranteed

FR865C achieves UL94 V0 flammability rating (2.5mm) and RoHS compliance, eliminating toxic hazards in electronics and meeting global environmental regulations.

Optimized Processing Efficiency

With high melt flow (30g/10min @220°C/10kg), it ensures fast, consistent molding—reducing cycle times and energy costs for complex parts.

Reliable Mechanical Performance

Balanced strength (40MPa tensile, 67MPa flexural) and impact resistance (18kJ/m² IZOD) ensure durable components under daily stress.

Suke FR865C ABS resin
Suke FR865C ABS resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top