Suke 3016 PC/ABS Resin Flame Retardant Grade
Suke 3016 is a premium PC/ABS blend offering superior impact strength and halogen-free safety. Perfect for electrical enclosures, durable office equipment, and router housings, it combines toughness with excellent processability for reliable, high-quality industrial components.
- Manufacturer: Suke Plastics
- Character: Halogen-free, High impact
- Application: Electrical &electronic, Office supplies, Router
Key technical data (ASTM)
- Material Safety: UL94 V0 (1.5mm thickness)
- Impact Strength: 60 KJ/m² (Izod Notched, 23°C)
- Flow Rate: 21 g/10min (260°C / 2.16 kg)
- Tensile Strength: 55 MPa
- Flexural Strength: 88 MPa
- Thermal Resistance: HDT 88°C (1.8MPa)
- Density: 1.18 g/cm³
- Mold Shrinkage: 0.4–0.8% (2mm thickness)
- Processing Temp: 230–270°C (Barrel), Max. 280°C
Download
Application
- Electrical & Electronic Components: Connectors, sockets, switch housings.
- Office Supplies: Printer panels, scanner covers, durable keyboard frames.
- Router & Networking Gear: Impact-resistant casings and structural parts.

Features & Benefits

Related Suke PC/ABS Products
Suke Plastics 3016GL PC ABS
Suke Plastics 3016NH PC ABS
Suke Plastics 3016NW PC ABS
Suke Plastics 3040 PC ABS
Suke Plastics 3020 PC ABS
Suke Plastics 3016 PC ABS
Suke Plastics D570 PC ABS Resin
Suke Plastics D555 PC ABS
Suke Plastics D535 PC ABS
Suke Plastics 1065 PC ABS
Suke Plastics 1045 PC ABS
Suke Plastics 1030 PC ABS
Advanced Manufacturing