Suke 3016GL PC/ABS Resin Flame Retardant Grade
Suke 3016GL is a halogen-free PC/ABS solution offering exceptional high fluidity for complex, thin-walled components. Engineered for demanding electrical, electronic, and consumer applications, it delivers reliable V0 flame retardancy, balanced toughness, and excellent processability, streamlining your production while meeting critical safety standards.
- Manufacturer: Suke Plastics
- Character: Halogen-free, High fluidity.
- Application: Electrical &electronic, Office supplies, Router.
Key technical data (ASTM)
- Density: 1.18 g/cm³
- Mold Shrinkage: 0.4 – 0.8% (2mm)
- Melt Flow Rate (MFR): 30 g/10min (260°C / 2.16 kg)
- Flammability (UL94): V0 @ 1.5mm
- Tensile Strength: 50 MPa
- Elongation at Break: 30%
- Flexural Strength: 90 MPa
- Flexural Modulus: 2100 MPa
- Izod Impact (Notched, 23°C): 50 KJ/m²
- HDT @ 1.8 MPa: 82°C
- Pre-Drying: 75-85°C for 3 hours (Critical!)
- Melt Temperature: ~250°C
- Max. Processing Temp: 270°C
- Mold Temperature: ~70°C
- Injection Pressure: 60-100 MPa
- Injection Speed: Medium-High (50-80)
Download
Application
- Electrical & Electronic Components: Housings for switches, connectors, sockets, power adapters, control boxes
- Office Equipment & Supplies: Printer components, scanner housings, keyboard frames, monitor bezels
- Networking Hardware: Router enclosures, modem casings, switch housings, and other telecom equipment parts

Features & Benefits

Related Suke PC/ABS resin Products
Suke Plastics 3016GL PC ABS
Suke Plastics 3016NH PC ABS
Suke Plastics 3016NW PC ABS
Suke Plastics 3040 PC ABS
Suke Plastics 3020 PC ABS
Suke Plastics 3016 PC ABS
Suke Plastics D570 PC ABS Resin
Suke Plastics D555 PC ABS
Suke Plastics D535 PC ABS
Suke Plastics 1065 PC ABS
Suke Plastics 1045 PC ABS
Suke Plastics 1030 PC ABS
Advanced Manufacturing