Formosa TAIRILAC® AE10EP ABS

Formosa Plastics TAIRILAC ANC160

TAIRILAC® AE10EP ABS Resin Jet Black Extrusion Grade

Tairilac AE10EP is a jet black extrusion-grade ABS resin. Optimized for extrusion molding, this high-rigidity material delivers exceptional impact resistance, making it ideal for industrial components requiring durability and structural integrity.

  • Manufacturer: Formosa Plastics (FCFC)
  • Character: Extrusion molding, Super high impact, High rigid
  • Application: Pipes
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (iSO)

  • Melt Flow Index: 4.9 g/10 min (220°C, 10kg)
  • Impact Strength: 48 kJ/m² (23°C, 4mm notch)
  • Tensile Strength: 37 MPa
  • Flexural Strength: 51 MPa
  • Heat Resistance: 86°C (1.8 MPa, unannealed)
  • Specific Gravity: 1.05
  • Pre-drying: 70–80°C × 2–3 hr

Features & Benefits

Super-High Impact Resistance

Tairilac AE10EP withstands heavy stress and shocks (48 kJ/m² per ISO 180), reducing cracks or breaks in high-impact environments like plumbing systems.

Optimized Extrusion Performance

Pre-dried at 70–80°C for 2–3 hours, it ensures smooth processing and minimizes defects for consistent, high-quality output.

Jet Black Aesthetic & Rigidity

With deep color stability and high flexural strength (51 MPa), it maintains structural integrity and visual appeal in visible applications.

FCFC Formosa TAIRILAC ABS Resin

Application

Pipes

Ideal for industrial and plumbing pipes requiring impact resistance, pressure tolerance, and long-term durability.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top