TAIRILAC® ANC160 ABS Self Extinguishing Grade
TAIRILAC ANC160 by Formosa Plastics is a flame retardant ABS resin. It’s great for making parts of electronic devices like LCD monitors and computers because it doesn’t catch fire easily. It has the best flame retardancy rating, stopping burning quickly. It’s also good with electricity and can handle heat up to 60°C without problems.
- Manufacturer: Formosa Plastics (FCFC)
- Character: Flame retardant
Key technical data (ISO)
- Flame Retardancy: UL 94 V-0 (2.5mm & 3.0mm) | IEC 60695-11-10 certified.
- Electrical Safety: Hot-Wire Ignition (HWI): PLC 2 (resists ignition); Arc Resistance: PLC 6 (excellent for high-voltage parts).
- Thermal Performance: RTI (Electrical/Mechanical/Impact): 60°C across all metrics.
- Heat Resistance: Vicat Softening Point @120°C
- Compliance: UL 746, ASTM D495, and IEC standards

Application
- Office Equipment Housings: TAIRILAC ANC160’s flame retardancy and PLC 0 HAI rating make it ideal for printers and copiers, preventing electrical fires in busy office environments.
- Consumer Electronics: Used in LCD monitor and TV casings, ANC160’s UL 94 V-0 rating ensures compliance with global safety standards while resisting heat from prolonged use.
- Industrial Machinery Components: Its thermal stability (RTI 60°C) and arc resistance suit high-amp industrial devices, reducing maintenance costs and downtime.

Tairilac® ANC160 Datasheet
| Self Extinguishing Grade FCFC TAIRILAC® ANC160 Data Sheet | ||||
| Product Description: Flame retardant | ||||
| Property | Unit | Test Method | Test Condition | Model ANC160 |
| Combustibility | UL-94 | File No. E162823 | v-0 2.5 mm | |
Tairilac® ANC160 UL Product iQ
| TAIRILAC® ANC160 UL Product iQ | ||
| File Number: E162823 | Acrylonitrile Butadiene Styrene (ABS), pellets | |
| Flammability | Value | Test Method |
| Flame Rating | UL 94 | |
| 2.5 mm, ALL | V-0 | IEC 60695-11-10, -20 |
| 3.0 mm, ALL | V-0 | |
| Electrical | Value | Test Method |
| Hot-wire Ignition (HWI) | UL 746 | |
| 2.5 mm | PLC 2 | |
| 3.0 mm | PLC 2 | |
| High Amp Arc Ignition (HAI) | UL 746 | |
| 2.5 mm | PLC 0 | |
| 3.0 mm | PLC 0 | |
| Comparative Tracking Index (CTI) | PLC 0 | UL 746 |
| High Voltage Arc Tracking Rate (HVTR) | PLC 0 | UL 746 |
| Arc Resistance | PLC 6 | ASTM D495 |
| Thermal | Value | Test Method |
| RTI Elec | UL 746 | |
| 2.5 mm | 60.0°C | |
| 3.0 mm | 60.0°C | |
| RTI Imp | UL 746 | |
| 2.5 mm | 60.0°C | |
| 3.0 mm | 60.0°C | |
| RTI Str | UL 746 | |
| 2.5 mm | 60.0°C | |
| 3.0 mm | 60.0°C | |
Related Tairilac® ABS Plastics
Formosa TAIRILAC® AG20GF ABS
Formosa TAIRILAC® AG16A1
Formosa TAIRILAC® AE10EP ABS
Formosa TAIRILAC® AX4100 ABS
Formosa TAIRILAC® ANC120 ABS
Formosa TAIRILAC® AE8700 ABS
Formosa TAIRILAC® AG10NP ABS
Formosa TAIRILAC® AE8000 ABS
Formosa TAIRILAC® AG10AP ABS
Formosa TAIRILAC® AG23AT ABS
Formosa TAIRILAC® ANC100 ABS
Formosa TAIRILAC® AX4300 ABS
Formosa TAIRILAC® AX4000
Formosa TAIRILAC® AF3535
Formosa TAIRILAC® AF3530 ABS
Formosa TAIRILAC® AF3560 ABS
Formosa TAIRILAC® AF3500 ABS
Formosa TAIRILAC® AG100H ABS
Advanced Manufacturing