TAIRIPRO® K8009 Impact Copolymer Injection Molding
TAIRIPRO K8009 is an impact-resistant polypropylene resin engineered for demanding industrial applications. Combining high impact strength (73–392 kJ/m²) and excellent fluidity (MFI 9 g/10min), it excels in automotive parts, battery cases, appliances, and furniture. Ideal for lightweight, durable components, this tairipro PP resin simplifies production while ensuring reliability in harsh conditions.
- Character: High impact strength, Good fluidity
- Application: Automotive parts, Battery case,Electrical appliances, Furniture
Key technical data (iSO)
- Melt Flow Index: 9 g/10min (230°C/2.16kg)
- Impact Strength: 73 kJ/m² (0°F) | 392 kJ/m² (73°F)
- Heat Deflection Temp: 110°C
- Tensile Strength: 22 MPa | Elongation: >200%
- Flammability Rating: UL 94 HB (1.5mm)
- Molding Shrinkage: 1.4–1.8%
- Processing Temp: 180–230°C (injection molding)
- Specific Gravity: 0.9 (lightweight design advantage)
Features & Benefits

Application
- Automotive Parts: Bumpers, dashboards, and under-hood components benefit from impact resistance and heat tolerance.
- Battery Cases: Safeguards EV and industrial batteries with durability and flame-retardant properties (HB rating).
- Electrical Appliances: Ideal for housings, connectors, and heat-resistant kitchenware.
- Furniture: Lightweight yet sturdy outdoor chairs, storage bins, and modular designs.

Related Tairipro® PP Plastics
FCFC TAIRIPRO® T2502 PP Resin
FCFC TAIRIPRO® T1202 PP Resin
FCFC TAIRIPRO® T1002 PP Resin
FCFC TAIRIPRO® S1803 PP Resin
FCFC TAIRIPRO® S1005 PP Resin
FCFC TAIRIPRO® S1003 PP Resin
FCFC TAIRIPRO® S1040 PP Resin
FCFC TAIRIPRO® S1019 PP Resin
FCFC TAIRIPRO® K2051 PP Resin
FCFC TAIRIPRO® K1525 PP Resin
FCFC TAIRIPRO® K1108 PP Resin
FCFC TAIRIPRO® K1080 PP Resin
FCFC TAIRIPRO® K1023 PP Resin
FCFC TAIRIPRO® K1011AG PP Resin
FCFC TAIRIPRO® F2011 PP Resin
FCFC TAIRIPRO® F2003 PP Resin
FCFC TAIRIPRO® F1611 PP Resin
FCFC TAIRIPRO® B1101 PP Resin
FCFC Formosa TAIRIPRO® T4002
FCFC Formosa TAIRIPRO® T3002
FCFC Formosa TAIRIPRO® F4008
FCFC Formosa TAIRIPRO® F4007
FCFC Formosa TAIRIPRO® F4006
FCFC Formosa TAIRIPRO® K4750
FCFC Formosa TAIRIPRO® K4715
FCFC Formosa TAIRIPRO® K4650
FCFC Formosa TAIRIPRO® K4515
FCFC Formosa TAIRIPRO® K4038
FCFC Formosa TAIRIPRO® T8002
FCFC Formosa TAIRIPRO® B8001A3
Advanced Manufacturing