FCFC Formosa TAIRIPRO® K8065

FCFC TAIRIPRO PP resin Impact Copolymer

TAIRIPRO® K8065 Impact Copolymer Injection Molding

TAIRIPRO K8065 is an impact copolymer polypropylene (PP) resin. With high fluidity, excellent impact strength (even at low temperatures), high stiffness, and low warpage, this material is ideal for injection-molded components requiring precision, structural integrity, and resistance to mechanical stress. Its balanced properties make it a versatile choice for industrial and consumer goods.

  • Character: High fluidity, Good impact strength, High Stiffness, Low warpage
  • Application: Washing machine, Storage boxes, Thin wall products
Please enable JavaScript in your browser to complete this form.
Click or drag files to this area to upload. You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ISO)

  • Melt Flow Rate: 65 g/10min (230°C/2.16kg, ASTM D-1238)
  • Heat Resistance: Heat deflection temperature of 115°C
  • Mechanical Strength: Tensile strength 240 kg/cm²; elongation >100%
  • Certifications: Food contact compliance (FDA 21 CFR), RoHS

Features & Benefits

Superior Flow for Complex Designs

The high melt flow index (65 g/10min) ensures effortless filling of intricate molds, reducing cycle times and enabling production of thin-walled or detailed parts like automotive panels and appliance housings.

Impact Resistance Across Temperatures

With an Izod impact strength of 9 kg·cm/cm at 23°C and 4.8 kg·cm/cm at -20°C, this resin withstands sudden shocks and harsh environments, making it suitable for outdoor storage containers or freezer components.

Stability with Minimal Warping

A flexural modulus of 12,500 kg/cm² and low molding shrinkage (1.4–1.8%) ensure dimensional accuracy, critical for tightly fitting parts like washing machine gears or industrial crate assemblies.

FCFC Formosa TAIRIPRO PP Impact Copolymer

Application

Washing Machine Components

It resists mechanical stress and moisture, ensuring long-lasting drum parts and housings.

Storage Boxes

It withstands stacking loads and temperature fluctuations, ideal for industrial or household containers.

Thin-Wall Products

High fluidity enables precise molding for lightweight packaging, disposable cutlery, and automotive trim.

Tairipro K8065 PP Resin application

Related Tairipro® PP Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity