TAIRIPRO® K8802 Impact Copolymer Injection Molding
TAIRIPRO® K8802 is a high-performance polypropylene (PP) impact copolymer resin engineered for demanding industrial applications. With exceptional impact strength, resistance to low-temperature brittleness, and a glossy finish, it excels in injection-molded products requiring durability and aesthetics. Ideal for suitcase components.
- Character: Hight impact strength,Excellent resistance to low temp. Brittleness, Good luster
- Application: Suitcase Parts
Key technical data (ISO)
- Melt Flow Index: 2 g/10 min (230°C, 2.16kg | ISO 1133)
- Tensile Strength: 270 kg/cm² (ASTM D-638) / 26.5 MPa (ISO 527)
- Flexural Modulus: 11,000 kg/cm² (ASTM D-790) / 1,078 MPa (ISO 178)
- Molding Shrinkage: 1.5–1.9% (23°C | FCFC Method)
- Heat Deflection Temperature: 105°C (0.45MPa | ASTM D-648)
- Flammability Rating: HB (UL 94)
Features & Benefits

Application

Related TAIRIPRO® PP Plastics
FCFC TAIRIPRO® T2502 PP Resin
FCFC TAIRIPRO® T1202 PP Resin
FCFC TAIRIPRO® T1002 PP Resin
FCFC TAIRIPRO® S1803 PP Resin
FCFC TAIRIPRO® S1005 PP Resin
FCFC TAIRIPRO® S1003 PP Resin
FCFC TAIRIPRO® S1040 PP Resin
FCFC TAIRIPRO® S1019 PP Resin
FCFC TAIRIPRO® K2051 PP Resin
FCFC TAIRIPRO® K1525 PP Resin
FCFC TAIRIPRO® K1108 PP Resin
FCFC TAIRIPRO® K1080 PP Resin
FCFC TAIRIPRO® K1023 PP Resin
FCFC TAIRIPRO® K1011AG PP Resin
FCFC TAIRIPRO® F2011 PP Resin
FCFC TAIRIPRO® F2003 PP Resin
FCFC TAIRIPRO® F1611 PP Resin
FCFC TAIRIPRO® B1101 PP Resin
FCFC Formosa TAIRIPRO® T4002
FCFC Formosa TAIRIPRO® T3002
FCFC Formosa TAIRIPRO® F4008
FCFC Formosa TAIRIPRO® F4007
FCFC Formosa TAIRIPRO® F4006
FCFC Formosa TAIRIPRO® K4750
FCFC Formosa TAIRIPRO® K4715
FCFC Formosa TAIRIPRO® K4650
FCFC Formosa TAIRIPRO® K4515
FCFC Formosa TAIRIPRO® K4038
FCFC Formosa TAIRIPRO® T8002
FCFC Formosa TAIRIPRO® B8001A3
Advanced Manufacturing