FCFC Formosa TAIRIPRO® T4002

FCFC TAIRIPRO PP resin Random Copolymer

TAIRIPRO® T4002 Random Copolymer PP Film Grade

TAIRIPRO T4002 is a high-performance PP random copolymer resin designed for extrusion and blow molding. Combining good transparency and excellent chemical resistance, it offers durability and versatility. T4002 ensures consistent quality across packaging, automotive, and consumer goods sectors.

  • Character: Good transparency, Good resistance to chemical
  • Application: Blow molding, sheet
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 1.6 g/10min (230°C, 2.16kg)
  • Impact Strength: 78 kJ/m² (23°C, notched)
  • Tensile Strength: 25 MPa
  • Flexural Modulus: 833 MPa
  • Heat Resistance: 85°C (0.455MPa load)
  • Molding Shrinkage: 1.5–2%
  • IZOD Impact Strength (23°C, Notched): 78 kJ/m²

Features & Benefits

Crystal-Clear Durability

With 85°C heat deflection temperature and >200% elongation, T4002 maintains structural integrity under stress, making it perfect for transparent containers exposed to heat or impact.

Chemical & Moisture Resistance

It resists acids, alkalis, and solvents, ensuring long-lasting performance in harsh environments like chemical storage tanks or automotive fluid components.

Easy Processing Flexibility

Optimized 1.6 g/10min melt flow rate allows smooth extrusion and blow molding, reducing energy consumption and production downtime.

FCFC Formosa TAIRIPRO PP Random Copolymer

Application

Blow Molding

Ideal for producing clear bottles, containers, and other hollow articles requiring transparency and chemical resistance, Automotive fuel tanks and air ducts.

Sheet Extrusion

Suitable for manufacturing transparent sheets used in packaging, signage, and protective barriers.

Tairipro T4002 PP Resin application

Related Tairipro® PP Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top