FCFC TAIRIPRO® F1611 PP Resin

FCFC TAIRIPRO PP resin Homopolymer

TAIRIPRO® F1611 Homopolymer PP Resin Blown Film Grade

TAIRIPRO F1611 is a homopolymer polypropylene resin engineered with high slip and anti-block properties. This versatile material delivers exceptional processing efficiency and reliability for demanding packaging solutions, backed by ISO-certified quality. Ideal for high-performance blown film applications.

  • Character: High slip, Anti-block
  • Application: packaging in General
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 10.5 g/10 min (230°C, 2.16 kg)
  • Tensile Strength: 35 MPa
  • Elongation at Break: >200%
  • Flexural Modulus: 1,500 MPa
  • Impact Strength: 27 kJ/m² (notched, 23°C)
  • Heat Deflection Temp: 115°C (0.455 MPa)
  • Specific Gravity: 0.9
  • Rockwell Hardness: R-100

Features & Benefits

Optimized Processing Efficiency

With an ISO 1133 melt flow rate of 10.5 g/10 min, F1611 ensures smooth extrusion and reduced energy consumption. Ideal for high-speed blown film lines.

Superior Film Performance

200% elongation at break (ISO 527) and 27 kJ/m² impact strength (ISO 180) prevent tearing during production. Reduces waste in packaging operations.

Safe & Easy Handling

Non-hazardous (GHS-exempt) and stable below 60°C. Simplifies storage and meets global safety standards.

FCFC Formosa TAIRIPRO PP Homopolymer

Application

Food Packaging Films

anti-block prevents layer sticking

Industrial Liners & Bags

high slip eases filling/sealing

Consumer Goods Wraps

tear resistance protects contents

Lightweight Protective Sheets

clarity + durability

Tairipro B1101 PP Resin application

Related TAIRIPRO® PP Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top