FCFC TAIRIPRO® F2011 PP Resin

FCFC TAIRIPRO PP resin Homopolymer

TAIRIPRO® F2011 Homopolymer PP Resin Film Grade

TAIRIPRO F2011 Homopolymer PP Resin is a high-performance polypropylene designed for precision film applications. Featuring middle slipping and exceptional clarity, this versatile resin delivers reliable processability and optical excellence for demanding packaging solutions. Ideal for extrusion and molding, it balances efficiency with end-product quality.

  • Character: Middle slipping, Good clarity
  • Application: CPP usage, Flexible & Rigid packaging
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 7 g/10 min (230°C, 2.16 kg)
  • Tensile Strength: 31 MPa | Elongation at Break: >200%
  • Impact Strength: 34 kJ/m² (23°C, notched)
  • Flexural Modulus: 1,274 MPa
  • Specific Gravity: 0.9
  • Rockwell Hardness: R-100
  • Processing Screw Temperature: 220–260°C
  • Processing Cooling Water: 30–40°C

Features & Benefits

Superior Optical Clarity

TAIRIPRO® F2011 offers crystal-clear transparency, enhancing product visibility for consumer packaging like food wraps or display films – no additives needed.

Balanced Processing Ease

Its middle slipping properties reduce friction during high-speed extrusion, minimizing downtime and ensuring smooth production of thin, uniform films.

Reliable Thermal Stability

With a high melting point (140–170°C) and heat deflection temperature (105°C), it withstands rigorous processing without degrading, maintaining consistency in output.

FCFC Formosa TAIRIPRO PP Homopolymer

Application

CPP Films

High-clarity cast polypropylene films for food packaging (e.g., snack bags, confectionery wraps).

Flexible Packaging

Pouches, laminates, and flow wraps requiring seal integrity and transparency.

Rigid Packaging

Containers, caps, and display boxes where stiffness and visual appeal are critical.

Tairipro F2011 PP Resin application

Related TAIRIPRO® PP Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity