FCFC TAIRIPRO® K1011AG PP Resin

FCFC TAIRIPRO PP resin Homopolymer

TAIRIPRO® K1011AG Homopolymer PP injection molding grade

TAIRIPRO K1011AG Homopolymer PP Resin delivers exceptional performance for demanding industrial applications. Engineered for long-term heat resistance (RTI 125°C), high stiffness, and superior surface luster, this k1011 polypropylene resin excels in precision injection molding. Ideal for durable electrical components requiring dimensional stability and aesthetic appeal.

  • Character: Long term heat resistance,High stiffness,Good luster
  • Application: Electric appliance parts, RTI=125℃
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 5 g/10 min (ISO 1133)
  • Tensile Strength: 7 MPa (ISO 527)
  • Impact Strength (Notched): 35 kJ/m² (ISO 180)
  • Flexural Modulus: 1,617 MPa (ISO 178)
  • Heat Deflection Temp.: 125°C (0.45 MPa) (ISO 75/A)
  • Molding Shrinkage: 1.4–1.8% (FCFC Method)
  • Flammability Rating HB (1.5–3.0 mm): UL 94
  • Specific Gravity: 0.9 (ISO 1183)

Features & Benefits

Reliable Heat Resistance

With a 125°C Relative Thermal Index (RTI), K1011AG withstands prolonged exposure to high temperatures without warping—critical for electrical housings near heat sources.

Superior Structural Rigidity

High flexural modulus (1,617 MPa) ensures exceptional stiffness, reducing deformation in load-bearing parts like appliance frames and connectors.

Premium Surface Finish

It delivers consistent, high-gloss surfaces directly from the mold—eliminating secondary polishing for cost-sensitive consumer goods.

FCFC Formosa TAIRIPRO PP Homopolymer

Application

Electric appliance parts

requiring long-term heat resistance (RTI = 125°C)

Connectors & Sockets

Resists deformation at 125°C continuous use.

Power Tool Components

HB flammability rating enhances safety.

Consumer Electronics

High-gloss finish for aesthetic casings.

Injection-molded parts

exposed to mechanical stress and elevated temperatures.

Tairipro K1011AG PP Resin application

Related TAIRIPRO® PP Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top