FCFC TAIRIPRO® K1023 PP Resin

FCFC TAIRIPRO PP resin Homopolymer

TAIRIPRO® K1023 Homopolymer PP injection molding grade

TAIRIPRO K1023 is a premium homopolymer polypropylene (PP) resin engineered by FORMOSA CHEMICALS & FIBRE CORPORATION (FCFC), Taiwan. With high fluidity, excellent stiffness, and superior surface luster, it delivers consistent performance for precision injection molding. Ideal for thin-walled components, consumer goods, and FDA-compliant applications.

  • Character: High fluidity, Good Stiffness, Good luster
  • Application: Thin wall parts,Housewares,Toys,meets the requirements of USP Plastic Class VI
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 25 g/10 min (ISO 1133)
  • Tensile Strength: 33 MPa (ISO 527)
  • Impact Strength (Notched): 25 kJ/m² (ISO 180)
  • Flexural Modulus: 1,372 MPa (ISO 178)
  • Heat Deflection Temp.: 110°C (0.45 MPa) (ISO 75/A)
  • Specific Gravity: 0.9 (ISO 1183)
  • Flammability Rating: HB (1.5mm & 3.0mm), UL 94

Features & Benefits

Exceptional Processing Efficiency

TAIRIPRO® K1023’s high melt flow index (25 g/10 min, ISO 1133) ensures rapid, uniform mold filling—reducing cycle times and energy costs for high-volume production.

Reliable Structural Integrity

Boasting a flexural modulus of 1,372 MPa (ISO 178), it provides outstanding rigidity and dimensional stability for durable parts that resist deformation under stress.

Premium Aesthetics & Safety

Delivers glossy, defect-free surfaces without post-processing. HB-rated flammability (UL 94) and USP Class VI compliance ensure safety for household, toy, and medical uses.

FCFC Formosa TAIRIPRO PP Homopolymer

Application

Thin-Wall Parts

Food containers, caps, and lightweight packaging.

Consumer Housewares

Storage bins, kitchen utensils, and appliance housings.

Toys & Childcare

Safe, impact-resistant components meeting global safety standards.

Medical Compliance

USP Class VI-certified for non-implant medical devices.

Tairipro K1023 PP Resin application

Related TAIRIPRO® PP Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top