FCFC TAIRIPRO® K1525 PP Resin

FCFC TAIRIPRO PP resin Homopolymer

TAIRIPRO® K1525 Homopolymer PP injection molding grade

TAIRIPRO K1525 is a premium homopolymer polypropylene resin engineered for high-performance injection molding. Combining high fluidity, rigidity, gloss, and transparency, this tairipro k1525 pp resin ensures effortless processing and exceptional end-product aesthetics. Ideal for demanding applications where clarity and structural integrity are critical.

  • Character: High fluidity, High Stiffness , Good luster, Good Transparency
  • Application: microwave containers, Food containers
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 25 g/10 min (ISO 1133, 230°C/2.16kg)
  • Impact Strength: 25 kJ/m² (ISO 180, notched)
  • Tensile Strength: 35 MPa | Elongation at Break: >50% (ISO 527)
  • Flexural Modulus: 1,764 MPa (ISO 178)
  • Heat Resistance: 125°C deflection temperature (ISO 75/A)
  • Shrinkage: 1.4–1.8% | Density: 0.9 g/cm³ (ISO 1183)
  • Flammability: HB (UL 94, 1.5–3.0mm)
  • Processing Screw Temperature: 200–290°C
  • Injection Pressure: 80–120 kg/cm²
  • Mold Temperature: 30–50°C

Features & Benefits

Superior Flow for Complex Molds

TAIRIPRO® K1525’s high melt flow index (25 g/10 min) fills intricate molds rapidly, minimizing cycle times and production costs while reducing material waste.

Exceptional Rigidity & Durability

With high stiffness (1,764 MPa flexural modulus) and impact strength, this Tairipro pp resin delivers warp-resistant parts that endure mechanical stress in harsh environments.

Premium Surface Finish

Excellent transparency and luster eliminate post-processing, creating visually appealing products like containers straight off the production line.

FCFC Formosa TAIRIPRO PP Homopolymer

Application

Microwave Containers

Withstands heat (125°C+) without warping.

Food Containers

Non-toxic, odorless, and maintains crystal-clear appearance.

Tairipro K1525 PP Resin application

Related TAIRIPRO® PP Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top