FCFC TAIRIPRO® T1202 PP Resin

FCFC TAIRIPRO PP resin Homopolymer

TAIRIPRO® T1202 Homopolymer PP Extrusion Grade

Tairipro T1202 is a homopolymer polypropylene (PP) resin engineered for blow molding applications. It delivers exceptional stiffness, heat resistance, and clarity—ideal for demanding industrial packaging, containers, and automotive parts. Optimized for extrusion processes, Tairipro PP resin ensures reliable performance and cost-efficiency.

  • Character: Blow molding
  • Application: high stiffness, heat resistance, clarity
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 1.6 g/10 min (ISO 1133, 230°C)
  • IZOD Impact Strength: 44 kJ/m² (ISO 180, 23°C)
  • Specific Gravity: 0.9
  • Tensile Strength: 380 kg/cm²
  • Heat Deflection Temp: 135°C
  • Molding Shrinkage: 1.5–1.9%
  • Processing Temp: 190–210°C (blow molding)

Features & Benefits

Superior Structural Rigidity

With a flexural modulus of 18,000 kg/cm², Tairipro T1202 resists deformation under stress—perfect for load-bearing containers like fuel tanks or industrial drums.

High-Temperature Resilience

It withstands temperatures up to 135°C (HDT), making it suitable for hot-filled packaging (e.g., food sauces) or automotive components near engines.

Crystal-Clear Visual Appeal

It offers excellent optical clarity for consumer packaging (e.g., transparent bottles), enhancing product visibility without sacrificing durability.

FCFC Formosa TAIRIPRO PP Homopolymer

Application

Rigid Packaging

Chemical drums, detergent bottles.

Hot-Fill Containers

Food jars, sauce bottles.

Automotive Reservoirs

Coolant tanks, windshield fluid containers.
Industrial Parts: Storage bins, pallets.

Consumer Goods

Transparent cosmetic tubes, healthcare packaging.

Tairipro T1202 PP Resin application

Related TAIRIPRO® PP Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top