Formosa TAIRILAC® AG15E1 ABS

Formosa Plastics TAIRILAC ANC160

TAIRILAC® AG15E1 ABS Resin General Purpose Grade

Tairilac AG15E1 is high-gloss, high-rigidity ABS resin engineered for precision injection molding. FCFC ABS Resin delivers exceptional surface aesthetics, impact resistance, and flow properties—ideal for consumer goods demanding durability and premium finishes.

  • Manufacturer: Formosa Plastics (FCFC)
  • Character: High gloss, High rigid
  • Application: Toys, Calculators, Phone,Clock housing,Stereo housing, Suitcase
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ISO)

  • Melt Flow Index: 25 g/10 min (220°C, 10kg)
  • Charpy Impact: 16 kJ/m² (23°C, notched)
  • Tensile Strength: 46 MPa
  • Flexural Modulus: 2,500 MPa
  • HDT @1.8MPa: 91°C (annealed)
  • Vicat Softening: 95°C
  • Flammability: HB (UL94, 1.6mm)
  • Mold Shrinkage: 0.4–0.7%
  • Processing Screw Temp: 190–230°C
  • Processing Pre-drying: 70–80°C × 2–3 hrs

Features & Benefits

Superior Impact Resistance

With 16 kJ/m² Charpy impact strength (ISO 179), Tairilac ABS AG15E1 withstands accidental drops and impacts, reducing breakage in consumer products.

Premium Surface Finish

High-gloss, painting-free surfaces save post-processing costs while maintaining consistent aesthetics for housings and visible components.

Excellent Flow for Complex Molds

High melt flow (25g/10min @220°C) ensures complete filling of intricate geometries, minimizing defects in thin-walled designs.

FCFC Formosa TAIRILAC ABS Resin

Application

Toys & Calculators

Scratch-resistant, non-brittle safety.

Phone/Clock Housings

Glossy finish, structural integrity.

Stereo Cases

Vibration resistance, aesthetic appeal.

Suitcases

Impact durability for travel stress.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top