FCFC Formosa TAIRIPRO® K7005AN

FCFC TAIRIPRO PP resin Impact Copolymer

TAIRIPRO® K7005AN Impact Copolymer Injection Molding

TAIRIPRO K7005AN is a high-performance polypropylene resin engineered for high impact strength and high stiffness. Designed for durability in demanding environments, this impact copolymer excels in automotive, furniture, and appliance manufacturing, offering reliability under stress and extreme conditions.

  • Character: High impact strength, High Stiffness
  • Application: Automotive parts, Furniture,Appliances
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Impact Strength (23°C): 392 kJ/m² (ISO 180)
  • Impact Strength (-20°C): 49 kJ/m² (ISO 180)
  • Stiffness: 1,372 MPa Flexural Modulus (ISO 178)
  • Heat Resistance: 120°C Heat Deflection Temperature (ISO 75/A)
  • Lightweight: Specific Gravity 0.9 (ISO 1183)
  • Flame Safety: UL94 HB Rating (1.5mm thickness)
  • Molding Shrinkage: 1.4–1.8% (optimized for precision)
  • Processing Temps: 180–230°C (energy-efficient molding)

Superior Impact Resistance

With 392 kJ/m² IZOD impact strength at 23°C (ISO 180), TAIRIPRO K7005AN prevents cracks in high-stress parts like automotive bumpers or appliance handles, even after repeated impacts.

Structural Stability Under Load

A flexural modulus of 1,372 MPa (ISO 178) ensures components like furniture frames or automotive panels retain shape under heavy loads, avoiding warping or deformation.

Fast, Efficient Processing

The melt flow index of 5 g/10 min (ISO 1133) enables smooth injection molding, reducing cycle times for complex parts like thin-walled appliance housings.

FCFC Formosa TAIRIPRO PP Impact Copolymer

Application

  • Automotive Parts: Bumpers, interior trim, and under-the-hood components requiring impact resistance and heat tolerance.
  • Furniture: Structural frames, chair bases, and storage bins needing rigidity and long-term durability.
  • Appliances: Washing machine panels, vacuum cleaner housings, and electrical enclosures demanding precision molding and flame safety.
Tairipro K7005AN PP Resin application

Related TAIRIPRO® PP Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top