TAIRIPRO K7009AH is a high-performance impact copolymer PP resin engineered for durability and heat resistance. With long-term thermal aging stability, high stiffness, and excellent impact strength, it’s ideal for demanding automotive and electrical components. Trusted by engineers for reliability under stress.

  • Character Description: Long term thermal aging, High stiffness, Good impact strength
  • Application: Electric appliance parts, Automotive parts,RTI=125℃
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 9 g/10 min (230°C/2.16kg)
  • Impact Strength: 108 kJ/m² at 23°C (ISO 180)
  • Heat Resistance: RTI 125°C (UL 746)
  • Molding Shrinkage: 1.4–1.8%
  • Screw Temperature: 180–230°C
  • Safety: HB flammability rating (UL 94)

Superior Impact Resistance

TAIRIPRO K7009AH delivers 45 kJ/m² at -18°C (ISO 180), ensuring parts like automotive bumpers or power tool housings resist cracking even in extreme conditions.

High Stiffness & Durability

A flexural modulus of 1,323 MPa (ISO 178) provides structural integrity for thin-walled components, reducing warpage in appliances or industrial containers.

Thermal Longevity

With an RTI (Relative Thermal Index) of 125°C, this tairipro PP resin withstands prolonged heat exposure, perfect for under-hood automotive parts or electrical connectors.

FCFC Formosa TAIRIPRO PP Impact Copolymer

Application

  • Electric Appliances: Housings for power tools, connectors, and circuit breakers.
  • Automotive: Under-hood components (e.g., battery trays, fan shrouds), interior trim.
  • High-Temperature Parts: Industrial containers, HVAC systems, and LED lighting housings.
Tairipro K7009AH PP Resin application

Related Tairipro® PP Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top