FCFC Formosa TAIRIPRO® K7025

FCFC TAIRIPRO PP resin Impact Copolymer

TAIRIPRO® K7025 PP Impact Copolymer Injection Molding

TAIRIPRO K7025 is an impact copolymer PP resin engineered for high-performance industrial applications. Combining high fluidity and exceptional impact strength, it simplifies complex molding processes while delivering durability. Ideal for appliances and automotive components.

  • Character: High fluidity, High impact strength
  • Application: Washing machine cylinder, Appliances
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 27 g/10min (ISO 1133)
  • IZOD Impact Strength: 78 kJ/m² (23°C, ISO 180)
  • Flexural Modulus: 1,372 MPa (ISO 178)
  • Molding Shrinkage: 1.4–1.8% (FCFC Method)
  • Processing Temp: 180–230°C (Injection Molding)
  • Safety Compliance: Non-hazardous (GHS), UL94 HB-rated.

Superior Flow for Faster Production

TAIRIPRO K7025’s high fluidity (Melt Flow Index: 27 g/10min) fills intricate molds effortlessly, reducing cycle times by up to 20%. Example: Perfect for thin-walled washing machine cylinders that require flawless surface finish and dimensional accuracy.

Unmatched Impact Resistance

With IZOD impact strength of 78 kJ/m² at room temperature, this tairipro pp resin withstands sudden shocks and repetitive stress. Example: Durable appliance housings that resist cracks during assembly or daily use.

Heat-Resistant & Dimensional Stability

A heat deflection temperature of 120°C ensures components retain shape under high heat. Example: Reliable performance in dishwasher parts exposed to steam and hot water.

FCFC Formosa TAIRIPRO PP Impact Copolymer

Application

  • Washing Machine Cylinders: High fluidity ensures smooth molding of lightweight, crack-resistant components.
  • Small & Large Appliances: Durable housings for microwaves, dishwashers, and refrigerators.
  • Automotive Interiors: Impact-resistant panels and trim parts.
  • Industrial Containers: Tough, heat-stable storage solutions.
Tairipro K7025 PP Resin application

Related Tairipro® PP Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top