FCFC Formosa TAIRIPRO® K8009

FCFC TAIRIPRO PP resin Impact Copolymer

TAIRIPRO® K8009 Impact Copolymer Injection Molding

TAIRIPRO K8009 is an impact-resistant polypropylene resin engineered for demanding industrial applications. Combining high impact strength (73–392 kJ/m²) and excellent fluidity (MFI 9 g/10min), it excels in automotive parts, battery cases, appliances, and furniture. Ideal for lightweight, durable components, this tairipro PP resin simplifies production while ensuring reliability in harsh conditions.

  • Character: High impact strength, Good fluidity
  • Application: Automotive parts, Battery case,Electrical appliances, Furniture
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (iSO)

  • Melt Flow Index: 9 g/10min (230°C/2.16kg)
  • Impact Strength: 73 kJ/m² (0°F) | 392 kJ/m² (73°F)
  • Heat Deflection Temp: 110°C
  • Tensile Strength: 22 MPa | Elongation: >200%
  • Flammability Rating: UL 94 HB (1.5mm)
  • Molding Shrinkage: 1.4–1.8%
  • Processing Temp: 180–230°C (injection molding)
  • Specific Gravity: 0.9 (lightweight design advantage)

Features & Benefits

Unmatched Impact Resistance

TAIRIPRO K8009 delivers exceptional toughness, with IZOD impact strength up to 392 kJ/m² at 73°F. Perfect for automotive bumpers or battery housings, it resists cracks and fractures even in sub-zero environments.

Effortless Moldability

With a melt flow index of 9 g/10min, this tairipro PP resin fills intricate molds smoothly, reducing cycle times and minimizing waste. Ideal for thin-walled electrical components or complex furniture designs.

Heat-Resistant Performance

It withstands temperatures up to 110°C (HDT), ensuring stability in heat-stressed applications like engine compartments or dishwasher-safe appliance parts.

FCFC Formosa TAIRIPRO PP Impact Copolymer

Application

  • Automotive Parts: Bumpers, dashboards, and under-hood components benefit from impact resistance and heat tolerance.
  • Battery Cases: Safeguards EV and industrial batteries with durability and flame-retardant properties (HB rating).
  • Electrical Appliances: Ideal for housings, connectors, and heat-resistant kitchenware.
  • Furniture: Lightweight yet sturdy outdoor chairs, storage bins, and modular designs.
Tairipro K8009 PP Resin application

Related Tairipro® PP Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top