FCFC Formosa TAIRIPRO® K8050

FCFC TAIRIPRO PP resin Impact Copolymer

TAIRIPRO® K8050 Impact Copolymer Injection Molding

TAIRIPRO® PP K8050 is an impact copolymer resin blending high fluidity (50 MFI), excellent impact strength, high stiffness, and low warpage. UL-94 HB, FDA, and RoHS certified, it optimizes thin-walled packaging, washing machine components, and rugged storage boxes, ensuring cost-efficiency and reliability for automotive, consumer, and industrial applications.

  • Character: High fluidity, Good impact strength, High Stiffness,Low warpage
  • Application: Washing machine,Storage boxes,Thin wall products
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 50 g/10 min @230°C/2.16kg (ASTM D-1238)
  • Impact Strength: 10 kg·cm/cm (23°C) / 5 kg·cm/cm (-20°C)
  • Tensile Strength: 240 kg/cm² (ASTM D-638)
  • Heat Resistance: HDT of 115°C (0.455 MPa)
  • Certifications: Complies with UL-94 HB, FDA, RoHS, and REACH SVHC requirements.
  • Density: 0.9 g/cm³

Features & Benefits

High Fluidity for Complex Molds

TAIRIPRO K8050’s superior melt flow (50 g/10 min) enables seamless filling of intricate molds, reducing cycle times and minimizing defects in thin-walled designs like containers or automotive panels.

Impact Resistance Across Temperatures

With IZOD impact strength of 10 kg·cm/cm at 23°C and 5 kg·cm/cm at -20°C, this resin withstands sudden shocks and low-temperature brittleness, ideal for washing machine components or outdoor storage boxes.

Dimensional Stability & Rigidity

A tensile strength of 240 kg/cm² and flexural modulus of 12,500 kg/cm² ensure minimal warpage and structural integrity, critical for precision parts requiring tight tolerances.

FCFC Formosa TAIRIPRO PP Impact Copolymer

Application

Washing Machine Components

It resists mechanical stress and moisture, ensuring long-lasting drum parts and housings.

Storage Boxes

It withstands stacking loads and temperature fluctuations, ideal for industrial or household containers.

Thin-Wall Products

High fluidity enables precise molding for lightweight packaging, disposable cutlery, and automotive trim.

Tairipro K8050 PP Resin application

Related Tairipro® PP Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top