TAIRIPRO® S1040 Homopolymer PP Multi-Filament Grade
TAIRIPRO® S1040 is a premium homopolymer polypropylene resin engineered for high-efficiency fiber production. Featuring controlled rheology, compact spinning compatibility, and anti-gas fading properties, it ensures consistent performance in demanding applications like nonwovens and fine denier fibers. Ideal for industrial-scale extrusion and molding.
- Character: Controlled rheology, Compact Spinning, Anti gas fading
- Application: Nonwoven, Fine Denier staple fiber
Key technical data (ISO)
- Melt Flow Index: 34 g/10 min (ISO 1133, 230°C/2.16 kg)
- Tensile Strength: 34 MPa (ISO 527)
- Elongation at Break: >50% (ISO 527)
- Flexural Modulus: 1,470 MPa (ISO 178)
- Impact Strength: 23 kJ/m² (ISO 180, notched)
- Heat Resistance: 110°C deflection temperature (ISO 75/A)
- Specific Gravity: 0.9 (ISO 1183)
- Hardness: R-103 Rockwell (ISO 2039-2)
Features & Benefits

Application

Related Tairipro® PP Plastics
FCFC TAIRIPRO® T2502 PP Resin
FCFC TAIRIPRO® T1202 PP Resin
FCFC TAIRIPRO® T1002 PP Resin
FCFC TAIRIPRO® S1803 PP Resin
FCFC TAIRIPRO® S1005 PP Resin
FCFC TAIRIPRO® S1003 PP Resin
FCFC TAIRIPRO® S1040 PP Resin
FCFC TAIRIPRO® S1019 PP Resin
FCFC TAIRIPRO® K2051 PP Resin
FCFC TAIRIPRO® K1525 PP Resin
FCFC TAIRIPRO® K1108 PP Resin
FCFC TAIRIPRO® K1080 PP Resin
FCFC TAIRIPRO® K1023 PP Resin
FCFC TAIRIPRO® K1011AG PP Resin
FCFC TAIRIPRO® F2011 PP Resin
FCFC TAIRIPRO® F2003 PP Resin
FCFC TAIRIPRO® F1611 PP Resin
FCFC TAIRIPRO® B1101 PP Resin
FCFC Formosa TAIRIPRO® T4002
FCFC Formosa TAIRIPRO® T3002
FCFC Formosa TAIRIPRO® F4008
FCFC Formosa TAIRIPRO® F4007
FCFC Formosa TAIRIPRO® F4006
FCFC Formosa TAIRIPRO® K4750
FCFC Formosa TAIRIPRO® K4715
FCFC Formosa TAIRIPRO® K4650
FCFC Formosa TAIRIPRO® K4515
FCFC Formosa TAIRIPRO® K4038
FCFC Formosa TAIRIPRO® T8002
FCFC Formosa TAIRIPRO® B8001A3
Advanced Manufacturing