TAIRIPRO® KP03B Impact Copolymer Injection Molding
TAIRIPRO® KP03B is a high-performance polypropylene (PP) impact copolymer resin. Combining high fluidity with excellent impact strength, this pellet-form material excels in injection molding processes, delivering consistent results for automotive components, durable storage solutions, and precision thin-wall products. Compliant with RoHS, UL94 HB, and REACH SVHC standards.
- Character: High fluidity, Hight impact strength
- Application: Bumper, Automotive parts, Thin wall products
Key technical data (ISO)
- Melt Flow Rate: 30 g/10min (230°C/2.16kg)
- Impact Strength: 49 kJ/m² (23°C), 36 kJ/m² (-20°C)
- Tensile Strength: 25 MPa
- Flexural Modulus: 1,323 MPa
- Molding Shrinkage: 1.4–1.8%
- Flame Rating: UL94 HB (1.5–3mm)
Features & Benefits

Application

Related TAIRIPRO® PP Plastics
FCFC TAIRIPRO® T2502 PP Resin
FCFC TAIRIPRO® T1202 PP Resin
FCFC TAIRIPRO® T1002 PP Resin
FCFC TAIRIPRO® S1803 PP Resin
FCFC TAIRIPRO® S1005 PP Resin
FCFC TAIRIPRO® S1003 PP Resin
FCFC TAIRIPRO® S1040 PP Resin
FCFC TAIRIPRO® S1019 PP Resin
FCFC TAIRIPRO® K2051 PP Resin
FCFC TAIRIPRO® K1525 PP Resin
FCFC TAIRIPRO® K1108 PP Resin
FCFC TAIRIPRO® K1080 PP Resin
FCFC TAIRIPRO® K1023 PP Resin
FCFC TAIRIPRO® K1011AG PP Resin
FCFC TAIRIPRO® F2011 PP Resin
FCFC TAIRIPRO® F2003 PP Resin
FCFC TAIRIPRO® F1611 PP Resin
FCFC TAIRIPRO® B1101 PP Resin
FCFC Formosa TAIRIPRO® T4002
FCFC Formosa TAIRIPRO® T3002
FCFC Formosa TAIRIPRO® F4008
FCFC Formosa TAIRIPRO® F4007
FCFC Formosa TAIRIPRO® F4006
FCFC Formosa TAIRIPRO® K4750
FCFC Formosa TAIRIPRO® K4715
FCFC Formosa TAIRIPRO® K4650
FCFC Formosa TAIRIPRO® K4515
FCFC Formosa TAIRIPRO® K4038
FCFC Formosa TAIRIPRO® T8002
FCFC Formosa TAIRIPRO® B8001A3
Advanced Manufacturing