FCFC Formosa TAIRIPRO® B8001A3

FCFC TAIRIPRO PP resin Impact Copolymer

TAIRIPRO® B8001A3 Impact Copolymer Injection Molding

With excellent impact strength and superior resistance to low-temperature brittleness, TAIRIPRO B8001A3 ensures reliability in harsh environments. Ideal for extrusion, blow molding, and thermoforming, this TAIRIPRO PP resin delivers consistent performance for automotive, construction, and cold-chain packaging applications.

  • Character: Excellent impact strength, Excellent resistance to low temp. brittleness
  • Application: PP-B pipe, Thermoforming sheet,Blow molding
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Impact Strength: 80 kJ/m² (23°C) / 11 kJ/m² (-20°C)
  • Melt Flow Index: 0.3 g/10 min
  • Tensile Strength: 26 MPa
  • Flexural Modulus: 1,178 MPa
  • Heat Deflection Temp.: 105°C
  • Molding Shrinkage: 1.5–1.9%
  • FDA-compliant, UL-94 HB flame-retardant rated

Features & Benefits

Unmatched Impact Resistance

B8001A3’s IZOD impact strength of 80 kJ/m² (ISO 180) prevents cracks in high-stress components like automotive bumpers or industrial containers, reducing part replacement costs.

Reliable in Freezing Conditions

With 11 kJ/m² impact strength at -20°C (ISO 180), this resin maintains integrity for cold-chain packaging, outdoor equipment, and refrigeration systems, eliminating brittleness risks.

Seamless Processing Flexibility

A low melt flow index of 0.3 g/10 min (ISO 1133) allows smooth extrusion, blow molding, and thermoforming, minimizing energy use and production downtime.

FCFC Formosa TAIRIPRO PP Impact Copolymer

Application

PP-B Pipes

Durable, chemical-resistant piping for industrial and plumbing systems.

Thermoforming Sheets:

High-strength trays for food packaging or automotive interior panels.

Blow-Molded Products:

Hollow parts like fuel tanks, containers, and chemical drums requiring impact resistance.

Tairipro B8001A3 PP Resin application

Related TAIRIPRO® PP Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top