FCFC TAIRIPRO® B1101 PP Resin

FCFC TAIRIPRO PP resin Homopolymer

TAIRIPRO® B1101 Homopolymer PP Extrusion Grade

TAIRIPRO B1101 is a high-performance homopolymer polypropylene resin engineered for extrusion and blow molding. With exceptional melt strength and deep-drawing capabilities, it creates complex, durable parts ideal for industrial applications—delivering reliability without compromising process efficiency.

  • Character: Excellent melt strength, Deep drawing
  • Application: Thermoforming Sheet, PP-H pipe, Tray, Blow molding
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index (260°C, 2.16 kg): 0.5 g/10 min
  • Impact Strength (Notched IZOD, 23°C): 69 kJ/m²
  • Tensile Strength: 35 MPa
  • Elongation at Break: >200%
  • Flexural Modulus: 1,421 MPa
  • Heat Deflection Temp (0.455 MPa): 110°C
  • Specific Gravity: 0.9
  • Hardness (Rockwell R): R-102

Features & Benefits

Excellent Melt Strength

It can ensure stable processing during deep-drawing operations, reducing tearing or thinning in complex shapes like automotive ducts or industrial containers.

Superior Impact Resistance

With 69 kJ/m² notched IZOD strength (ISO 180), it withstands physical stress, ideal for trays, pipes, and blow-molded products requiring durability.

High-Temperature Stability

It can maintain integrity at 110°C (HDT, ISO 75/A), ensuring dimensional reliability in thermoforming sheets or hot-fill packaging.

FCFC Formosa TAIRIPRO PP Homopolymer

Application

Thermoforming Sheets

Food trays, medical packaging.

PP-H Pipes

Chemical-resistant industrial pipelines.

Blow Molding

Fuel tanks, automotive fluid reservoirs.

Industrial Trays

Heavy-duty material-handling containers.

Tairipro B1101 PP Resin application

Related TAIRIPRO® PP Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top