FCFC Formosa TAIRIPRO® KP03B

FCFC TAIRIPRO PP resin Impact Copolymer

TAIRIPRO® KP03B Impact Copolymer Injection Molding

TAIRIPRO® KP03B is a high-performance polypropylene (PP) impact copolymer resin. Combining high fluidity with excellent impact strength, this pellet-form material excels in injection molding processes, delivering consistent results for automotive components, durable storage solutions, and precision thin-wall products. Compliant with RoHS, UL94 HB, and REACH SVHC standards.

  • Character: High fluidity, Hight impact strength
  • Application: Bumper, Automotive parts, Thin wall products
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Rate: 30 g/10min (230°C/2.16kg)
  • Impact Strength: 49 kJ/m² (23°C), 36 kJ/m² (-20°C)
  • Tensile Strength: 25 MPa
  • Flexural Modulus: 1,323 MPa
  • Molding Shrinkage: 1.4–1.8%
  • Flame Rating: UL94 HB (1.5–3mm)

Features & Benefits

Superior Molding Efficiency

With a melt flow index of 30 g/10min (ISO 1133), KP03B flows effortlessly into complex molds, reducing cycle times by 15–20% and minimizing energy consumption. Ideal for intricate geometries like automotive dash panels.

Unmatched Durability

It achieves 49 kJ/m² impact resistance at 23°C (ISO 180), ensuring toughness for heavy-duty storage boxes and shock-prone automotive under-the-hood parts. Maintains performance even at -20°C.

Heat-Resistant Performance

It boasts a heat deflection temperature of 115°C (ISO 75), preventing deformation in high-temperature environments such as automotive engine compartments or sterilizable containers.

FCFC Formosa TAIRIPRO PP Impact Copolymer

Application

Thin-Wall Products

Warping in delicate designs. Food packaging and disposable medical trays with consistent wall thickness (0.5–1mm).

ThinIndustrial Storage Boxes-Wal

Crack resistance during rough handling. Heavy-duty containers for logistics, retaining shape and strength after repeated drops.

Automotive Parts

Reducing weight while meeting crash safety standards. Bumper fascias, door trims, and interior panels benefit from KP03B’s impact resistance and heat tolerance.

Tairipro KP03B PP Resin application

Related TAIRIPRO® PP Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top